Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of titanium foil sheet in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Introduction
1. Titanium foil sheet is a thin metal strip made of pure titanium and titanium alloy, it is common in coil and thickness varies from 0.02~0.5mm, wide according to the customer's request and stock size.
2. Basic information
Grade: Gr1, Gr2, Gr5, Gr12 etc.
Purity: ≥99.5%
Density: ≥ 4.51g/cm3
Thickness: 0.02~0.5mm
Wide: 5~600mm
Standards: ASTMB265
3. Manufacture process of titanium foil
Titanium material with a thickness of 3.8 ~ 4.2mm is reduced to 0.01 ~ 0.05mm through cold rolling, by selecting titanium material with thicker thickness, the elongation of the titanium strip is increased to more than 36% after multiple cold rolling.
Detail Shows


4. Titanium foil sheet for the high-frequency sound film is made of titanium coil through rolling, cleaning, tension straightening, annealing, and other steps. It has high strength, good treble front effect, long service life, wide frequency response, and can improve distortion.
Ultra-thin titanium foil for sound film, the size has 25 core, 34 core, 38 core, 44 core, 51 core, 72 core, 74 core, 75 core, 99 core.
Stamping Cup: model: 1304, 1308, 1907, 1204, 1004 metal cup
5. Titanium foil can be used not only for loudspeakers and tweeter films but also for precision accessories, outdoor stoves, batteries, chemical fillers, sealing materials, bone implantation, etc.
6. As a professional titanium foil supplier, we can provide not only cp titanium foil but also titanium alloy foil such as Gr5 titanium 6al4v foil, Gr12 titanium foil, common use Gr1 titanium foil sheet stock, thickness from 0.02~0.5mm, for detail titanium foil price, pls send us an email for quotations or contact us by messages online.
7. Inspeciton and test
we can provide material test certification together with goods, 3rd party material, and physical test support, reach and Rohs tests are also available.
Hot Tags: titanium foil sheet, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ASTMB265 3 7105 UNS R53400 Gr12 Titanium Foil, Lightweight Titanium Foil For Stove Pipe