Titanium Mesh
Behind Every Drop of Clean Water, There's a Strong Mesh
Corrosion-resistant anode substrate titanium mesh
Focusing on titanium mesh processing and sales, our product range covers various titanium mesh products such as titanium mesh, titanium woven mesh, stamped titanium mesh, etc.
We have advanced production equipment and a technical team to meet customers' diverse needs and strict quality standards. Our titanium mesh products are widely used in aerospace, the chemical industry, electronics, environmental protection, and other fields, providing customers with reliable technical support and product solutions.
Characteristics of Titanium Mesh
Corrosion resistance: Titanium has excellent corrosion resistance and can be used for a long time in various chemical environments. Therefore, titanium mesh is often used in fields such as the chemical industry, marine engineering, and petroleum industries that require corrosion-resistant materials.
Lightweight: Titanium is a lightweight metal, and titanium mesh has a lower density than other metal meshes, making it suitable for applications that require weight reduction.
-
Titanium Screen MeshTitanium screen mesh is a durable, lightweight, and corrosion-resistant material that has a wide range of applications in various industries.Add to Inquiry
-
Gr1 Expanded Titanium Metal MeshTitanium Expanded Metal Mesh. 1. Ti expanded metal. 2. 3x6, 4x8, 5x10, 6x12 etc. 3. Diamond metal mesh. 4. ASTM B265, ASTM F67, and ASTM F136Add to Inquiry
-
Titanium Sintering Filter SheetTitanium Sintered Powder Filter Sheet. Sintering Titanium Filter Sheet. Sintered Titanium Porous Filter Sheets. Ti sintered metal microporous sheet. Titanium porous sintered metal sheet. porousAdd to Inquiry
-
Titanium wire mesh filter bagtitanium wire mesh bag. titanium wire mesh screen. titanium wire mesh basket. titanium wire mesh manufacturer. titanium woven wire meshAdd to Inquiry
-
Titanium Wire Mesh DemisterTitanium demister. Titanium mesh demister. Titanium wire mesh demister padsAdd to Inquiry
-
Grade 1 Titanium Wire MeshTitanium mesh screen. 1. UNS No.UNS R50250. 2. Grade: Gr1. 3. Type: titanium woven wire mesh; Titanium woven mesh.Add to Inquiry
-
Gr1 Diamond Titanium MeshDiamond titanium mesh. Titanium mesh plate. Stamped titanium mesh. UNS R50250 titanium meshAdd to Inquiry
Tel: +86-917-3664600
Fax: +86-917-3664600
Email: tina@tmsalloy.com
Add: No.11 South of Baoti Road, Baoji City, Shaanxi Province, P.R. China.
Common specifications of titanium mesh
-
Mesh hole Size: Usually described by the size of the mesh, for example, 1/4 inch, 1/2 inch, etc. The size in millimeters may also be used.
-
Wire Diameter: Indicates the diameter of titanium wire. Commonly used wire diameters range from 0.01 mm to several millimeters.
-
Mesh Size: Describes the overall size of the titanium grid, usually expressed in length and width, for example, 1 meter × 2 meters, 4 feet × 8 feet, etc.
-
Surface Finish: Titanium mesh may undergo different surface treatments, such as polishing, pickling, etc., to meet the requirements of specific applications.

Different Titanium Mesh

Diamond titanium mesh is usually made by stamping or cutting titanium sheets, and can be made into mesh structures of various shapes and sizes.
Features: Stamped titanium mesh usually has a relatively regular grid structure, and the hole size, shape, and arrangement can be customized according to specific design requirements.
Application: Common uses include industrial applications such as filtration, screening, and isolation, and it can also be used in decoration, construction, and other fields.

Titanium wire mesh is a mesh structure woven from titanium wire, similar to the woven structure of cloth.
Features: Titanium woven wire mesh is soft and elastic, can be stretched and shaped as needed, and has good plasticity.
Application: Common uses include filtration, isolation, protection, and other fields. It is especially suitable for applications that require softness and breathability, such as medical devices, filters, etc.
Applications of Titanium Mesh
electrochemical industry
One of the most important applications of titanium mesh is in the electrochemical industry. It is commonly used as a substrate for dimensionally stable anodes (DSA), including ruthenium-iridium and iridium-tantalum oxide-coated titanium mesh anodes. These products are widely applied in chlor-alkali electrolysis, electroplating, electrowinning, seawater electrolysis, wastewater treatment, and hydrogen production. Titanium mesh is also used in filtration and separation systems, including chemical filter elements, industrial screens, wire mesh demisters, and mist eliminators, where corrosion resistance and structural stability are essential.
Marine engineering and seawater treatment
Titanium mesh is valued for its excellent resistance to chloride-containing environments. Typical applications include seawater filtration, desalination equipment, electrolysis systems, and corrosion-resistant electrode structures. Selecting the appropriate mesh structure, opening size, wire diameter, and surface coating according to specific operating conditions helps ensure optimal performance and long-term service life.

FAQ
Q: What are the commonly used specifications of titanium woven mesh?
Pore size: The pore size of titanium woven mesh can vary according to specific needs. Common pore sizes include:
Small pore size: often used for fine filtration, screening, and isolation.
Medium pore size: suitable for general filtration and isolation applications.
Large Aperture: For applications such as ventilation, protection,n, and decoration.
Wire diameter: The wire diameter of titanium braided mesh can vary according to strength requirements and usage scenarios. Common wire diameters include:
Filament Diameter: For lightweight applications and fine filtration.
Medium Wire Diameter: Commonly used for general filtration and protection.
Coarse Wire Diameter: For applications requiring higher strength and durability.
Q: How do woven and expanded titanium mesh differ in application?
Q: What are the common specifications of expanded diamond titanium mesh?
A: The common specifications of diamond titanium mesh are 3x6, 4x8, 5x10, 6x12, 7x13mm, thickness 0.6 0.8 1.0 1.2 1.5 2.0mm, etc., and the maximum width is within 1500mm.
Q: What is the common width of woven titanium mesh?
A: The common specifications of woven titanium mesh are 40 mesh, 60 mesh, 80 mesh, 100 mesh, 150 mesh, etc. The spot width is 1000mm, the length is unlimited, and it can be shipped in rolls.
Q: Why is titanium mesh widely used as an anode substrate?
A: Titanium mesh is widely used as an anode substrate because it combines excellent corrosion resistance, high strength-to-weight ratio, open structural design, and compatibility with MMO coatings. These characteristics make it a reliable substrate for dimensionally stable anodes used in chlor-alkali electrolysis, seawater treatment, electroplating, and other industrial electrochemical processes.
For industrial buyers, selecting the right titanium mesh requires consideration of mesh opening, wire thickness, coating composition, and operating conditions. Grade 1 titanium expanded mesh is a common choice for MMO-coated anodes.
Q: How is titanium mesh used in electrochemical processes?
A: Titanium mesh plays an important role in modern electrochemical processes, especially in chlor-alkali production, seawater electrolysis, electroplating, electrowinning, and industrial wastewater treatment. Its excellent corrosion resistance, open structure, and compatibility with MMO coatings make it a preferred substrate for many dimensionally stable anodes.
As a titanium mesh manufacturer and supplier, we can provide titanium mesh in expanded and woven structures, with customized mesh openings, thicknesses, dimensions, and coating options to meet different industrial electrochemical requirements.
Q: What type of titanium mesh is suitable for chlor-alkali electrolysis?
A: Grade 1 expanded titanium mesh coated with Ru-Ir mixed metal oxides is a widely used solution for chlor-alkali electrolysis. Its open structure promotes electrolyte circulation and gas release, while its catalytic coating facilitates efficient chlorine evolution.
When purchasing titanium mesh for chlor-alkali applications, buyers should pay particular attention to mesh opening, substrate thickness, coating composition, and operating current density.
Q: How is woven titanium mesh used in gas-liquid separation?
A: Woven titanium mesh plays an important role in industrial gas-liquid separation, particularly in wire mesh demisters, mist eliminators, chemical absorption towers, acid mist removal systems, and petrochemical processing equipment. Its excellent corrosion resistance, lightweight structure, and flexible weaving design make it suitable for demanding environments where conventional stainless steel mesh may have a shorter service life.
Q: Can titanium mesh be used in sulfuric acid processing equipment?
A: Titanium mesh can be used in certain sulfuric acid processing applications, but it should not be considered universally resistant to sulfuric acid. Grade 1 titanium mesh may be suitable for dilute acid at relatively low temperatures, while Grade 7 and Grade 12 may provide better corrosion resistance under selected more demanding conditions.
For industrial filtration, demister pads, and chemical separation equipment, choosing the appropriate titanium grade is essential to ensure reliable performance and long service life. When sulfuric acid concentration or temperature is high, alternative materials such as tantalum or suitable nickel-based alloys may need to be evaluated.
Q: How does titanium mesh improve electrolysis efficiency in water treatment?
A: Titanium mesh improves electrolysis efficiency in water treatment through its open structure, large available electrode surface area, good electrolyte permeability, and compatibility with catalytic coatings. These properties help improve mass transfer, facilitate gas bubble removal, and support stable electrochemical reactions.
For industrial wastewater treatment, seawater disinfection, and electrochemical oxidation, selecting the right mesh opening, wire diameter, and surface coating is essential to achieving reliable treatment performance and longer electrode service life.
As a professional titanium mesh manufacturer and supplier, we can provide Grade 1 titanium mesh in expanded and woven structures, with customized dimensions and specifications for industrial electrochemical water treatment systems.
Q: How is titanium mesh used in marine corrosion protection systems?
A: Titanium mesh plays an important role in marine corrosion protection systems, particularly in impressed current cathodic protection, offshore structure protection, seawater pipeline protection, and marine anti-fouling equipment.
With its excellent corrosion resistance, lightweight structure, and compatibility with MMO coatings, expanded titanium mesh provides a reliable substrate for long-life electrochemical anodes. Compared with conventional consumable anodes, MMO-coated titanium mesh offers low consumption, stable dimensions, and adjustable protective current.
Q: How do wire diameter and mesh count affect titanium mesh performance?
A: Wire diameter and mesh count jointly determine the performance of woven titanium mesh. Thicker wires generally improve mechanical strength but reduce open area, while higher mesh counts create smaller openings and support finer filtration, often at the expense of flow capacity.
For industrial buyers, the best specification is not necessarily the mesh with the smallest openings or thickest wires. It is the combination that balances filtration accuracy, flow rate, mechanical strength, and service conditions.
Contact information:
Tel: +86-0917- 3664600
WhatsApp: +8618791798690
Baoji Fairy Titanium Industry Co., Ltd. is one of the most professional titanium mesh manufacturers and suppliers in China, featured by quality products and low price. Please rest assured to buy or wholesale bulk customized titanium mesh made in China here from our factory.
Titanium Screen Mesh, Titanium Expanded Metal Mesh