ASTMF67 ASTMF136 Biocompatible Titanium Strip For Medical

ASTMF67 ASTMF136 Biocompatible Titanium Strip For Medical

Ti Strip ASTMF67
Pure Ti Ribbon
Titanium strip coil
Medical Titanium strip coil
Titanium medical strip foil
Medical Grade 1 Titanium Strip
Pure titanium strip ASTMF67
Ti strip foil for implantable medical
Precision titanium strip for Medical Implants
Medical grade titanium strip
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of astmf67 astmf136 biocompatible titanium strip for medical in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

1. Titanium strip for medical is titanium sheet coil and foil which is wide below 600mm, it has low iron and oxygen, good biocompatibility, and can be used for medical devices and medical implants.

2. Titanium strip for medical size and standards

Grade: Gr1 Gr4 Gr5ELI Gr23

Thick: 0.05~0.3mm, 0.3~0.6mm

Wide: 10~600mm

Standards: ASTMF67, ASTMF136

Surface: cold rolling bright surface

titanium strip for medical for sale
titanium strip for medical price

3. Feature of titanium strip for medical

Titanium strips for medical applications are usually made from high-quality, medical-grade titanium. It is used in various medical devices and instruments where superior strength, corrosion resistance, and biocompatibility are essential properties. Below are some details regarding the characteristics of titanium strips for medical purposes:

Biocompatibility: Titanium is an extremely biocompatible material, which means it does not trigger any adverse biological responses when it is implanted into a patient's body. This makes it an ideal material for medical implants and prosthetics.

Corrosion-resistant: Titanium is highly resistant to corrosion from bodily fluids, acids, and alkalis, which makes it an ideal material for medical devices and implants that need to be durable and long-lasting.

High strength-to-weight ratio: Titanium has an exceptional strength-to-weight ratio, which means it is strong and durable while still being lightweight. This property makes titanium an excellent choice for medical devices where both durability and weight are essential.

Non-magnetic: Titanium is non-magnetic, which makes it ideal for magnetic resonance imaging (MRI) scans. It also allows for the use of titanium in devices requiring a non-magnetic property.

Machinability: With the advancement of technology, titanium can now be machined to precise specifications, making it easier to manufacture custom implants and medical devices.

4. The chemical compositions of titanium strips for medical applications according to ASTMF67

UNSGradeNCHFeOTi
UNS R50250Gr10.030.080.0150.20 0.18balance
UNS R50400Gr20.030.080.0150.30 0.25balance
UNS R50550Gr30.050.080.0150.30 0.35balance
UNS R50700Gr40.050.080.0150.50 0.40 balance

titanium strip for medical in stock

5. The mechanical property of pure titanium strips for medical applications according to ASTMF67

Gradetensile strength yield strength Elongation (%)
Gr1240170~31024
Gr2345275~45020
Gr3450380~55018
Gr4550483~65515

6. 3rd party test report of Gr1 titanium strip for medical applications

SGS, TUV, 3rd party material test supported, RoHS, reach also available for your choice, stable quality, and fast delivery, professional export package, contact sales@tmsalloy.com to buy titanium strip for medical now.

ASTMF67 gr1 titanium strip 0.3
gr1 titanium strip for medical 0.3mm

Hot Tags: astmf67 astmf136 biocompatible titanium strip for medical, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ASTMB265 3 7105 UNS R53400 Gr12 Titanium Foil, Lightweight Titanium Foil For Stove Pipe