Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of astmb265 gr5 gr7 gr9 gr12 titanium alloy sheet in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Introduction
1. Titanium alloy sheet is a type of metal sheet made of many titanium alloys, including Gr5, Gr7, Gr12, and others. It is an alloy composed of titanium and other elements, the most commonly used are Gr5 and Gr12.
2. Basic information
Grade: Gr5 Gr7 Gr9 Gr12 etc.
Size: 1000x2000, 1220x2440, 1500x3000 etc
Thickness: 0.5~80mm
Standards: ASTM B265,ASTM F136,AMS4928
Titanium alloy has two kinds of homogeneous and heterogeneous crystals: close-packed hexagonal structure below 882 ℃ α Titanium, and body-centered cubic above 882 ℃ β Titanium.
Alloy elements can be divided into three types according to their influence on phase transformation temperature:
① Steady α
Aluminum, carbon, oxygen, and nitrogen are examples of stable elements that elevate the phase transition temperature. Aluminum is the principal alloying element of titanium alloy. It has an obvious effect on improving the strength at room temperature and high temperature, reducing the specific gravity, and increasing the elastic modulus of the alloy.
② Steady β
The elements that decrease the phase transition temperature are β stable elements, which can be divided into isomorphic and eutectoid types. The former includes molybdenum, niobium, vanadium, etc. The latter include copper, iron, chromium, manganese, silicon, etc.
③ The elements that have a small effect on the phase transition temperature are neutral elements, such as zirconium, tin, and so on.
Oxygen, nitrogen, carbon, and hydrogen are the major impurities in titanium alloys. Oxygen and nitrogen have a large solubility in the α phase, which has an outstanding strengthening effect on titanium alloy but reduces the plasticity. It is generally stipulated that the contents of oxygen and nitrogen in titanium are less than 0.15 ~ 0.2% and 0.04 ~ 0.05% respectively. In this phase, hydrogen solubility is quite low. A titanium alloy that has too much hydrogen dissolved in it will produce hydride and become brittle. Generally, the hydrogen content is controlled below 0.015% in titanium alloy. The dissolution of hydrogen in titanium is reversible and can be eliminated by vacuum annealing.
Detail Shows


3. Titanium alloy has low density, high specific strength and stiffness, good corrosion resistance, high-temperature mechanical properties, fatigue resistance and creep resistance, and excellent comprehensive properties. It is a new type of structural material with great development potential and application prospects. It is widely used in the manufacturing of military products such as aerospace, ships, and weapons. It also has great application potential in the automotive, chemical, and energy industries.
4. Titanium alloy sheet has many excellent characteristics, which are mainly reflected in the following aspects:
-
High strength. Titanium alloy has high strength. Its tensile strength is 686-1176mpa, while its density is only about 60% of that of steel, so its specific strength is very high.
-
High hardness. Titanium alloy (annealed state) hardness is 32-38 HRC
-
Low elastic modulus. The elastic modulus of titanium alloy (annealed state) is 1.078 × 10-1.176 × 10MPa, about half of that of steel and stainless steel.
-
Excellent high and low-temperature performance. Titanium alloy can still preserve good mechanical properties at high temperatures. Its heat resistance is much higher than aluminum alloy, and its working temperature range is wide. At present, the working temperature of new heat-resistant titanium alloy can reach 550-600 ℃; At low temperatures, the strength of titanium alloy is higher than that at normal temperatures and has good toughness. Low-temperature titanium alloy can maintain good toughness at - 253 ℃.
5. Titanium alloy plate strength yield and elongation according to ASTMB265 standards.
| Grade |
Tensile Strength, min |
Yield Strength, 0.2 % Offset |
Elongation in 2 in. or 50 mm, min, % |
| 5 | 895 | 828 | 10 |
| 7 | 345 | 275~450 | 20 |
| 9 | 620 | 483 | 15 |
| 12 | 483 | 345 | 18 |
6. As a reputable titanium sheet supplier, we provide 6al4v titanium sheet, Gr7 (TiPd alloy) sheet, and Gr12 (Ti0.3mo0.8ni) sheet in stock, as well as the ability to order other alloys like Gr6 (Ti5al2.5sn) and BT20 (Ti6.5al1mo1v2zr). Except for the raw material, we can also supply titanium alloy sheet metal finished products, such as laser cutting, water jet cutting, and CNC machining parts according to drawings.
Contact us
Tel: +86-0917- 3664600
Whatsapp: +8618791798690
Email: sales@tmsalloy.com
tina@tmsalloy.com
Hot Tags: astmb265 gr5 gr7 gr9 gr12 titanium alloy sheet, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Sintered Porous Plate 1Mm Thickness Titanium Porous Metal Sintered Plate, ASTMB265 3 7105 UNS R53400 Gr12 Titanium Sheet, ASTMB265 Ti 0 2Pd Gr11 Titanium Plate, CT23755 87 Ti 5AL 2 5Sn Gr6 BT5 1 Titanium Plate, ASTMB265 Ti 0 05Pd Gr16 Titanium Sheet, ASTMB265 Ti 0 05Pd Gr17 Titanium Plate