Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of gr5 titanium wire on spool in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Introduction
1. Alpha-beta titanium alloy, or Ti6Al4V, is used to make Gr5 Titanium Wire On Spool, a type of metal wire with good durability at low temperatures.
2. Product Details
Grades include Gr5 ELI, Gr23, Ti6Al4V, Ti-6Al-4V, etc.
Measurements: OD57.0mm
Types include straight, in coil, etc.
MOQ: 5kg
Packaging information: Plywood case lined with foam, or as requested by the client
3. Titanium wire on a spool made of Ti-6Al-4V Gr5 has the benefits of both titanium alloys. It features a straightforward manufacturing technique and great resistance to seawater corrosion. It can be welded, cold- and hot-formed, and quenched and aged to reinforce it.
4. Titanium Gr. 5 Wire size variations according to AWSA5.16
| specified diameter in. | coils of wire on spools | cut straight length |
| 0.020~0.045 | ±0.001 | ±0.0015 |
| 0.045~0.062 | ±0.0015 | ±0.002 |
| 0.062~0.090 | ±0.002 | ±0.0025 |
| 0.090~0.187 | ±0.003 | ±0.003 |
| 0.187~0.25 | ±0.004 | ±0.004 |
Detail Shows
titanium wire on spool |
titanium wire supplier |
5. At present, Gr5 titanium wire is mainly used to weld various titanium alloy equipment, welding pipes, etc, it is also used to make fasteners, and load-bearing Due to its excellent all-around performance, Gr5 titanium wire is currently used mostly to weld different titanium alloy equipment, welding pipes, etc. It is also used to create fasteners, load-bearing parts, springs, etc., springs, etc. due to its good comprehensive performance.
Gr5 titanium wire |
buy Gr5 titanium wire |
6. Why pick us?
As a reputable manufacturer of titanium wire, we keep some common grades in stock, including Gr5 titanium wire on spools, Gr1 titanium filler wire, Gr12 titanium wires in coils, and Gr7 titanium welding wire. We can also order other grades, which are strictly produced in accordance with standards and packaged with care in plastic bags, boxes, and wooden cases.


Hot Tags: gr5 titanium wire on spool, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, AWSA5 16 ERTi17 Grade17 Titanium Welding Wires, Titanium Wire For Anodizing, Black Surface Titanium Gr1 Wire In Spool For Wire Mesh Making, ERTi 2 Erti 7 Erti 12 Titanium Mig Wire, ERTi 1 ER Ti 2 ER Ti 5 ER Ti 7 ER Ti 9 ER Ti 12 Titanium Filler Wire ASTMB863