Ti-0.2Pd UNS R52400 DIN 3.7235 Gr7 Titanium Plate

Ti-0.2Pd UNS R52400 DIN 3.7235 Gr7 Titanium Plate

Ti Gr7 3.7235
UNS R52400 Titanium Grade 7 Plate
Titanium Grade 7 Sheet
B265 Titanium Grade 7 Sheet
Gr7 3.7235 plates Titanium ASTM B265 Gr 7 Plate
Alloy Grade 7 Sheets ASTM B265
0.12~0.25%Pd
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of ti-0.2pd uns r52400 din 3.7235 gr7 titanium plate in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

Products Introduction

1. Gr7 titanium plate is also called TiPd alloy sheet, which contains 0.12 to 0.25% palladium, the small quantity of palladium added gives it enhanced crevice corrosion resistance at low temperatures.

2. Basic Information

3.7235 Gr7 titanium plate chemical composition:

Grade

N

C

H

Fe

O

Al

V

Pa

Mo

Ni

Ti

Gr 7

0.03

0.08

0.015

0.30

0.25

/

/

0.12~0.25

/

/

bal

Gr7 titanium plate tensile properties:

Grade

Tensile strength(min)

Yield strength(min)

Elongation (%)

Ksi

MPa

Ksi

MPa

Gr 7

50

345

40

275

20

Detail Shows

Gr7 titanium plate price

Gr7 titanium plate

Gr7 titanium plate supplier

Ti0.2Pd alloy plate

3. What are the Gr7 titanium plate applications?

Grade 7 titanium was mainly developed for use in the chemical industry. They offer the same excellent properties as pure titanium grades together with improved corrosion resistance, especially in chloride-containing media. With the development of science and technology and the depletion of terrestrial resources, human development and utilization of the ocean have been put on the agenda. Gr7 titanium plate has excellent corrosion resistance to seawater and is widely used in seawater desalination, ships, marine thermal energy development, and seabed resource mining.

Due to the characteristics of titanium Grade 7, they have unique advantages in the application of ships and marine equipment, so they are widely used in nuclear submarines, deep submersibles, atomic energy icebreakers, hydrofoils, hovercraft, and minesweepers. As well as propellers, seawater pipelines, condensers, heat exchangers, etc.

4. Comparison of chlorine ion resistance between pure titanium and Gr7 titanium alloy

The density of seawater is usually less than 5%. According to long-term experiments and actual applications, it is believed that pure titanium can be safely used in seawater below 120℃, but crevice corrosion may occur if the temperature rises. Ti-Pd alloy (Ti-0.2Pd, Gr7) can be used in high-temperature pressurized seawater at 260 degrees.

In different concentrations of sodium chloride solution, magnesium chloride solution, and calcium chloride solution. Titanium-palladium alloys and titanium-nickel-molybdenum alloys are more resistant to chloride than pure titanium.

5. What do we have of Gr7 titanium plate stock?

GradeThickness(mm)Size(mm)
Grade7 1.01000x2000
Grade7 1.21000x2000
Grade7 1.51000x2000
Grade7 2.01000x2000
Grade7 2.51000x2000
Grade7 3.01000x2000
Grade7 4.01000x2000
Grade7 6.01000x2000
Grade7 8.01000x2000
Grade7 10.01000x2000

6. Why choose us

We, a leading Gr7 titanium plate supplier in Baoji, have an R&D, manufacturing, and sales service team with rich professional background knowledge, and some Gr7 titanium plate stock. "Confidence, speed, effect" is our action policy, and the team's learning ability and continuous improvement of ability are our services. We are also willing to improve and strengthen our team under the trust and supervision of customers.

Hot Tags: ti-0.2pd uns r52400 din 3.7235 gr7 titanium plate, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, CT23755 87 Ti 5AL 2 5Sn Gr6 BT5 1 Titanium Plate, ASTMB265 Ti 0 05Pd Gr16 Titanium Sheet, ASTMB265 3 7105 UNS R53400 Gr12 Titanium Sheet, ASTMB265 Ti 0 2Pd Gr11 Titanium Plate, Sintered Porous Plate 1Mm Thickness Titanium Porous Metal Sintered Plate, ASTMB265 Ti 0 05Pd Gr17 Titanium Plate

Send Inquiry

(0/10)

clearall