ASME SB-265 UNS R54520 Gr6 Titanium Plate

ASME SB-265 UNS R54520 Gr6 Titanium Plate

Ti5al2.5sn plate
UNS R54520
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of asme sb-265 uns r54520 gr6 titanium plate in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

Products Introduction

1. Gr6 titanium plate is also known as Ti-5Al-2.5Sn, which contains 5% aluminum and 2.5% tin, it is used in airframes and jet engines due to its good weldability, stability, and strength.

2. Basic Information

Grade: Gr6 BT5 Ti-5Al-2.5V

Shape: rectangular, square, or circular (upon customers request)

Certification: ISO 9001: 2008

Minimum Order Quantity/Weight: 1 pc

Service area: Asia, America, Europe, Africa, Russia, and India.

Detail Shows

Gr6 titanium plate

Gr6 titanium plate

Ti5al2.5sn plate

Ti5al2.5sn plate

3. Gr6 Titanium characteristic

  • High Strength Titanium

  • High-Temperature Stability

  • Good Corrosion Resistance

  • Good Creep Resistance

4. Gr6 titanium plate has medium strength and sufficient plasticity in the annealed state and has good welding performance. It can be used below 500°C. When the content of interstitial impurity elements (oxygen, hydrogen, nitrogen, etc.) is extremely low, even at ultra-low temperatures, it still has good toughness and comprehensive mechanical properties. It is an excellent ultra-low temperature alloy and is most widely used.

5. Gr6 titanium plate chemical and physical properties

chemical compositions

chemical elementsNCHFeOAlTinResiduals max eachResiduals max total
Gr60.030.080.0150.50.24.0~6.02.0~3.00.10.4

Mechanical properties

Gradetensile strength Mpayield strength Mpaelongation
Gr682879310

6. Our advantage

We are a professional titanium metal supplier, Gr6 titanium plate supplier, and there are a large number of titanium plates in stock. We have established long-term and good cooperative relations with major logistics companies to ensure that the goods arrive at the destination quickly, on time, and safely. We are committed to fully understanding the needs and preferences of customers, and tailor-made professional products for customers.

Hot Tags: asme sb-265 uns r54520 gr6 titanium plate, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ASTMB265 Ti 0 05Pd Gr17 Titanium Plate, Sintered Porous Plate 1Mm Thickness Titanium Porous Metal Sintered Plate, ASTMB265 Ti 0 05Pd Gr16 Titanium Sheet, ASTMB265 3 7105 UNS R53400 Gr12 Titanium Sheet, CT23755 87 Ti 5AL 2 5Sn Gr6 BT5 1 Titanium Plate, ASTMB265 Ti 0 2Pd Gr11 Titanium Plate