Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of titanium rectangular tube in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Introduction
1. The square and rectangular cold-formed hollow titanium tube, which is made by rolling the round tube into a rectangle tube, is another name for it.
2. Fundamental Details
Square Tubing Grade 2 Specification
Grades: Gr2 through Gr5
4M in length or as ordered
Square titanium tube Dimensions: 40x40x3 or as requested
A 10mm wall thickness
ASME SB337, ASTM B337, and ASTM B 338
Detail Shows


3. Rectangular titanium tubes have a variety of applications. Exhaust pipes, heat exchangers, boilers, burners, furnaces, and condenser parts are just a few examples of high-heat applications that use titanium. Additional application areas include the power industry, petrochemical industry, natural gas processing facilities, specialty chemical industry, etc.
| Product name | Titanium square pipe |
| Standard | ASTM B861,ASTM B338,ASME SB861,ASME SB338 |
| Material | Pure titanium/Titanium alloy |
| Grade | Gr1,Gr2,Gr5,Gr7,Gr9,Gr10,Gr12 |
| Feature | Fine Corrosion Resistance/Light |
| Application | Industrial, Heating Exchanging, Condenser, Medical, Chemical, Aerospace, Oil, Sports, Bike, etc. |
| Surface | Pickling, polished |
| Packaging | Ply-wooden case, carton box |
| Shape | Round/Square/Rectangle |
| Supply Ability | 500 Ton/Tons per Month |


4. Size of titanium square pipes
| Thick-walled square tube specification(mm) | Thick wall rectangular tube specification(mm) | ||
| 16×16×0.4~1.5 | 380×380×8.0~30.0 | 10×20×0.6~1.5 | 250×150×6~12.0 |
| 18×18×0.4~1.5 | 400×400×8.0~30.0 | 14×21×0.6~1.5 | 250×100×6~12.0 |
| 20×20×0.4~1.5 | 420×420×10.0~30.0 | 15×30×1.5~1.5 | 250×200×6~30.0 |
| 25×25×0.6~2.0 | 450×450×10.0~30.0 | 15×38×0.6~1.5 | 300×150×6~30.0 |
| 30×30×0.6~4.0 | 480×480×10.0~30.0 | 20×30×0.6~2.0 | 300×200×6~30.0 |
| 34×34×1.0~2.0 | 500×500×10.0~30.0 | 20×40×0.8~2.0 | 300×250×6~30.0 |
| 35×35×1.0~4.0 | The other specifications | 20×50×1.0~2.0 | 400×250×8~30.0 |
| 38×38×1.0~4.0 | 550×550×10.0~40.0 | 22×35×0.9~2.0 | 400×300×8~30.0 |
| 40×40×1.0~4.5 | 600×600×10.0~40.0 | 25×40×0.9~3.75 | 450×200×8~30.0 |
| 44×44×1.0~4.5 | 700×700×10.0~40.0 | 25×65×1.0~2.0 | 450×250×8~30.0 |
| 45×45×1.0~5.0 | 800×800×10.0~50.0 | 30×40×1.0~3.75 | 400×300×8~30.0 |
| 50×50×1.0~5.0 | 900×900×10.0~50.0 | 30×45×1.0~3.75 | 400×350×8~30.0 |
| 60×60×1.5~5.0 | 1000×1000×10.0~50.0 | 30×50×1.0~4.0 | 500×200×10~30.0 |
| 70×70×2.0~6.0 | 30×60×1.0~4.5 | 500×250×10~30.0 | |
| 75×75×2.0~6.0 | 40×50×1.0~4.5 | 500×300×10~30.0 | |
| 80×80×2.0~6.0 | 40×60×1.0~5.0 | 500×350×10~30.0 | |
| 85×85×2.0~6.0 | 40×80×1.5~5.0 | 500×400×10~30.0 | |
| 95×95×2.0~8.0 | 40×100×2.0~5.0 | 500×450×10~30.0 | |
| 100×100×2.0~8.0 | 50×60×2.0~5.0 | The other specifications | |
| 120×120×4.0~8.0 | 50×80×2.0~5.0 | 600×200×10~28.0 | |
| 150×150×6.0~10.0 | 50×100×2.0~8.0 | 600×400×10~28.0 | |
| 180×180×6.0~12.0 | 60×80×2.0~6.0 | 600×500×10~28.0 | |
| 200×200×6.0~30.0 | 80×100×2.0~8.0 | 800×400×10~28.0 | |
| 220×220×6.0~30.0 | 120×60×2.5~10.0 | 800×600×10~28.0 | |
| 250×250×6.0~30.0 | 120×80×2.5~10.0 | 800×700×10~28.0 | |
| 280×280×6.0~30.0 | 150×100×2.5~12.0 | 1000×400×10~28.0 | |
| 300×300×8.0~30.0 | 180×150×2.5~12.0 | 1000×500×10~28.0 | |
| 320×320×8.0~30.0 | 200×100×4~12.0 | 1000×600×10~28.0 | |
| 350×350×8.0~30.0 | 200×150×4~12.0 | 1000×800×10~28 | |
Hot Tags: titanium rectangular tube, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, 30 45 90 Titanium Mandrel Bends, ASTM B338 Gr2 Titanium U Shaped Tube, Titanium Rectangular Tubing