UNS R56400 TA6V ASTMB348 Gr5 6al4v Titanium Rod

UNS R56400 TA6V ASTMB348 Gr5 6al4v Titanium Rod

UNS R56400 titanium
Corresponding Russian grade BT6
Corresponding German Garde DIN3.7165
Corresponding French Garde TA6V
MOQ 5KG for stock size, 100kg for ordered size
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of uns r56400 ta6v astmb348 gr5 6al4v titanium rod in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

Products Introduction

1. Aluminum and vanadium are added to the titanium alloy used to make 6al4v Titanium Rod. This material has very high corrosion resistance. It typically has a density of 4.51g/cm3, which is only 60% of steel.

2. Basic Information

Titanium bar ASTMB348 products in various sizes, shapes, and types.

Shape: round, flat, rectangle, square, etc.

Sizes for GR5 titanium rods include 5mm to 100mm in diameter, 100mm to 3000mm in length, and customizable lengths.

Detail Shows

timascus round bar

Gr5 titanium bar

Grade 5 Round Bar

Grade 5 Round Bar ASTMB348

3. What are the properties and chemical makeup of the 6al4v titanium rod?

Ti-6Al-4V and Ti 6-4 rods are other names for 6al4v titanium rods. ti-6al-4v-Eli should not be confused with it (grade 23). It is the most commonly used alloy. Its chemical composition consists of residual titanium, 6% aluminum, 4% vanadium, 0.25% (maximum) iron, and 0.2% (maximum) oxygen. Its strength is comparable to that of commercially pure titanium (grades 1-4), and it shares the same stiffness and thermal characteristics with grade 5 (except thermal conductivity, which is approximately 60% lower). Heat treatability is one of its numerous benefits. The qualities of strength, corrosion resistance, weldability, and manufacturability are all present in this grade in the ideal proportions.

1 kilo titanium bar

Titanium bar

titanium alloy bar

Titanium alloy bar

 

4. 6al4v titanium rod applications

Stronger than many steel alloy structural bars are several high-strength titanium alloys. Therefore, compared to other metal structural materials, 6al4v titanium rods have substantially greater specific strength (strength/density) and can be used to create pieces with high strength units, good stiffness, and lightweight. The grade of titanium alloy with the greatest utility is this one. It is commonly utilized for shafts, bolts, screws, and other components of structures.

6al4v titanium rod for sale

5. Why choose us?

As a high-quality 6al4v titanium rod manufacturer, we also have some similar grades of Gr5 6al4v, such as:

Ti-6Al-4V, Ti-6Al-4V ELI, Ti-6Al-4V SP, Ti-6Al-4V ELI SP (USA)

BT-6, BT-6C, BT-6К, BT-6КТ (Russia);

IMI-318, IMI-318ELI (UK);

TiAl6V4 (Germany); T-A6V (France); SAT-64 (Japan).

To contact us and purchase titanium rods right away, go to sales@tmsalloy.com.

FAQ

Q: 1. What is the composition of the 6al4v Titanium Rod?

A: According to ASTMB348 standard, the composition of Ti6AI-4V Titanium Rod is as follows
Aluminum 5.50 to 6.75%
Vanadium 3.50 to 4.50%
Oxygen (max) 0.020%
Iron (max) 0.40%
Carbon (max) 0.10%
Nitrogen 0.05%
Hydrogen (max) 0.015%
Others, total (max) 0.40%
*Others, each (max) = 0.1%
Titanium Others

Q: 2. What is the price of TA6V 6al4v Titanium material?

A: The price of the TA6V 6al4v Titanium Rod varies according to the outer diameter, and the price varies according to the fixed length or random length, specifically ranging from 120~230RMB/KG.

Contact information:

Tel: +86-0917- 3664600

Whatsapp: +8618791798690

Email: sales@tmsalloy.com
tina@tmsalloy.com

Hot Tags: uns r56400 ta6v astmb348 gr5 6al4v titanium rod, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ASTMF136 Gr5ELI Gr23 Medical Titanium Rods, Precision Titanium Round Bar Rod Ti 6Al 4V ELI, 10mm TA6V Grade 5 Titanium Rod, Precision Titanium Round Bar Rod Ti-6Al-4V ELI, Titanium Rectangular Bar Or Rec Bar, Timascus Rod Damascus Titanium Rod

Send Inquiry

(0/10)

clearall