ASTM B265 UNS R56400 TA6V Gr5 Titanium Plate

ASTM B265 UNS R56400 TA6V Gr5 Titanium Plate

6al4v titanium plate
1. UNS R56400 TA6V
2. Alpha-beta (α-β) titanium alloy
3. MOQ 1PCS or 1KG
4. 1000X2000mm or 1220 1250 1500mm wide
5. High strength and corrosion resistance
6. ASTMB265
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of astm b265 uns r56400 ta6v gr5 titanium plate in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

Products Introduction

1. Gr5 titanium plate, also known as Ti6Al4V, TA6V, or Ti 6-4, is the most commonly used alloy.

2. Product information

Titanium plate size: T x W x L (mm)

Thickness (4.1-60.0) x Wide (400-3000) x Length (1000-4000)

Thickness (0.3-4.0) x Wide (400-1500) x Length (1000-3000)

Product surface Pickling surface, water-polished surface, shiny bright surface
No cracks, peeling, oxide scale, crushing, or alkali washing traces on the surface
Product section Water cutting, shearing cutting, milling surface, laser cutting, wire cutting
Product raw materials High-quality titanium sponge ingot

3. Titanium Gr 5 plate chemical and physical features

Chemical composition:

Grade

N

C

H

Fe

O

Al

V

Pa

Mo

Ni

Ti

Gr 5

0.05

0.08

0.015

0.40

0.20

5.5~6.75

3.5~4.5

/

/

/

bal

Tensile properties:

Grade

Tensile strength(min)

Yield strength(min)

Elongation (%)

Ksi

Ksi

MPa

Ksi

MPa

5

130

895

120

828

10

4. Gr5 titanium plate performance

It has good machining performance and requires the use of carbide tools, large cutting volume, slow speed, and sufficient cooling. Good corrosion resistance and good thermal stability. It is suitable for long-term working parts below 400℃.

Detail Shows

titanium plate cost

6al4v titanium plate

Gr5 0.6 titanium sheet

titanium alloy plate

5. What is the application of the titanium Gr5 plate?

Titanium Grade 5 is found as the most used alloy in many areas.

- Aerospace and Aircraft

- sports equipment

- Medical industry

- Chemical Industry

ti plate ti5al2.5sn plate

6al4v titanium plate

ti0.3mo0.8ni titanium block

6al4v titanium block

6. Titanium other applications

Titanium and its alloys are used in the general industry to make electrodes in the electrolysis industry, condensers in power stations, heaters for petroleum refining and seawater desalination, and environmental pollution control devices. Gr5 titanium plates have become a kind of corrosion-resistant structural material. In addition, it is also used in the production of hydrogen storage materials and shape memory alloys.

7. Titanium alloy grade types

There are hundreds of titanium alloys in the world; the most famous are Ti-6Al-4V, Ti-5Al-2.5Sn, Ti-2Al-2.5Zr, and 20-30 types. 32Mo, Ti-Mo-Ni, Ti-Pd, SP-700, Ti-6242, Ti-10-5-3, Ti-1023, BT9, BT20, IMI829, IMI834, etc.

8. Our Package and Service

titanium sheet
titanium plate
3.0mm titanium plate

9. Our advantages:

We have a large amount of inventory. As a high-quality Gr5 titanium plate supplier, we can provide samples that can be processed and customized according to drawings, and can provide third-party inspection reports.

FAQ

Q: 1. Is grade 5 titanium good?

A: The density of grade 5 titanium is only about 4.5g/cm³. The grade 5 titanium plate is lighter but stronger than steel and other metal alloys.

Q: 2. What is the difference between the Gr2 and Gr5 titanium plates?

A: Gr2 titanium plate is widely used in chemical pressure vessels, seawater treatment equipment, shipbuilding, and other fields. Due to its good corrosion resistance and processing performance, the Gr2 titanium plate has a wide range of applications in industry and marine engineering.
Gr5 titanium plate is often used in aviation engine parts, high-temperature furnaces, and chemical equipment due to its excellent corrosion resistance and high strength.
Price and market supply
The Gr2 titanium plate has a relatively low price and sufficient market supply, making it suitable for large-scale production and general industrial applications.
Gr5 titanium plate has a higher price and relatively less market supply, and is mainly used in high-end and special application fields.
Gr2 and Gr5 titanium plates differ in composition, performance, and application areas. You can choose the right material according to your specific needs.

Q: 3. Is the Gr5 Titanium Plate in stock?

A: Gr5 Titanium Plate is in stock in all specifications, with thicknesses ranging from 0.5 to 80mm, commonly used widths of 1000mm and 1250mm, and lengths ranging from 2000 to 4000mm. Customized sizes are supported.

Q: 4. Can the Gr5 Titanium Plate be cut?

A: Gr5 Titanium Plate can be cut in half or cut according to customer drawings. Special customized sizes are available, and the construction period is 10 to 20 days, depending on the quantity.

Contact information:

Tel: +86-0917- 3664600

WhatsApp: +8618791798690

Email: sales@tmsalloy.com
tina@tmsalloy.com

Hot Tags: astm b265 uns r56400 ta6v gr5 titanium plate, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ASTMB265 Ti 0 2Pd Gr11 Titanium Plate, CT23755 87 Ti 5AL 2 5Sn Gr6 BT5 1 Titanium Plate, ASTMB265 Ti 0 05Pd Gr16 Titanium Sheet, ASTMB265 Ti 0 05Pd Gr17 Titanium Plate, Sintered Porous Plate 1Mm Thickness Titanium Porous Metal Sintered Plate, ASTMB265 3 7105 UNS R53400 Gr12 Titanium Sheet

Send Inquiry

(0/10)

clearall