Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of astm b265 uns r50400 3.7035 gr2 titanium sheet in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Introduction
1. A metal sheet manufactured of titanium grade 2 is known as a "gr2 titanium sheet," and the American standards are ASTM B265, ASTM F136, ASTM F67, and AMS4928.
2. Informational details:
US Grade: BT1-00, BT1-0, etc.; Gr1, Gr2, Gr3, Gr5, Gr7, Gr11, Gr12, etc.
Standard Russian grades include BT1-00, BT1-0, BT1-2, etc.
Size of a titanium sheet: T, W, and L (mm)
Thickness: 4.1-60.0mm
Length: 1000-4000mm x Width: 400-3000mm a hot roll
A thin layer of titanium 0.3-4.0 mm in thickness, 400-1500 mm in width, and 1000-3000 mm in length.
Hardness: HB150-HB340
| product name | Titanium and titanium alloy plate | thickness | 0.3-60MM |
| product material | Pure titanium, titanium alloy | Width length | Can be cut and customized |
| Product Grade | Gr1/Gr2/Gr12/Gr9/Gr5 etc. | applications | Industrial, medical |
| Supply status | Hot-working, cold-working, annealing, solid solution | Supply standard | ASTMB265, ASTMF136, ASTMF67 etc. |
3. Aviation, chemical, petroleum, manufacturing, medicinal, and other industries use titanium sheet metal.
One of the primary anti-corrosion materials in chemical equipment is titanium metal, which has established its anti-corrosion position in such equipment.
Detail Shows


4. Procedure for producing titanium sheets
Hot forging is the process of forging above the temperature at which metal recrystallizes.
While hot rolling of the Gr2 titanium sheet is done at a temperature higher than the recrystallization temperature, cold rolling is rolling done at the plastic deformation temperature.
The act of progressively raising a metal's temperature to a predetermined level, holding it there for a sufficient amount of time, and then swiftly cooling it is known as annealing (usually slow cooling, sometimes controlled cooling).
Pickling: To get rid of oxides and other coatings on the metal surface, submerge the parts in a solution of hydrofluoric acid and nitric acid. It is the intermediate treatment or pretreatment of electroplating, rolling, enamel, and other processes.

5. What are the other main applications for Gr2 titanium sheets?
After years of marketing, titanium and its alloys are now widely employed as a superior corrosion-resistant construction material in the chemical industry. The original soda ash and caustic soda businesses were the first to use titanium machinery. At this time, organic synthesis, dyes, inorganic salts, pesticides, chlorate, ammonium chloride, urea, and other industries have joined them.
The results of the heat exchanger survey showed that titanium heat exchangers accounted for 57%, titanium anodes accounted for 20%, titanium vessels accounted for 16%, and others accounted for 7%. In the chemical industry, "two alkalis" are the main ones, and titanium heat exchangers are used the most in chemical equipment.

6. Our advantages
As a professional titanium sheet supplier, pure titanium sheet, BT1-0 titanium plate, Gr5 titanium sheet (6al4v sheet TA6Vsheet), and Grade 2 titanium sheet stock. Since the company's inception, it has devoted a lot of time to focusing on the titanium metal market, experiencing multi-industry and multi-process corrosion-resistant solutions, gaining a wealth of product design and production experience, and continuing to innovate to draw clients to a variety of services and experiences. Contact us at sales@tmsalloy.com for quick delivery and excellent service to learn how much titanium sheet costs.
FAQ
Q: 1. What is the UNS number for Gr2 titanium?
Q: 2. Is Grade 2 titanium sheet bulletproof?
Q: 3. What specifications of Gr2 Titanium Sheet are in stock?
Q: 4. Is there a minimum order quantity for the Gr2 Titanium Sheet?
Contact information:
Tel: +86-0917- 3664600
Whatsapp: +8618791798690
Email: sales@tmsalloy.com
tina@tmsalloy.com
Hot Tags: astm b265 uns r50400 3.7035 gr2 titanium sheet, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ASTMB265 Ti 0 05Pd Gr16 Titanium Sheet, CT23755 87 Ti 5AL 2 5Sn Gr6 BT5 1 Titanium Plate, ASTMB265 3 7105 UNS R53400 Gr12 Titanium Sheet, Sintered Porous Plate 1Mm Thickness Titanium Porous Metal Sintered Plate, ASTMB265 Ti 0 2Pd Gr11 Titanium Plate, ASTMB265 Ti 0 05Pd Gr17 Titanium Plate