High Purity ASTMB348 Gr1 Titanium Bar

High Purity ASTMB348 Gr1 Titanium Bar

High Purity
Pure Titanium
ASTMB348
MOQ 10KG
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of high purity astmb348 gr1 titanium bar in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

1. Product Introduction

Gr1 titanium bar is a solid bar made of 99.5% titanium with a silver-white bright surface. It is made of pure titanium Grade 1, often used in aerospace, medical and chemical applications. These bars possess a low density, high strength, excellent corrosion resistance, and good weldability. 

2. Basic Information

Titanium bar Shape: Round, Square, and Rectangular

Dimensions: Custom-made size available

Titanium rod production status:

Hot processing state (R)

Cold working state (Y)

Annealing state (M)

3. Gr1 titanium bar chemical and mechanical properties according to ASTMB348

chemical elements N C H Fe O Residuals max each Residuals max total
Grade1 0.03 0.08 0.015 0.2 0.18 0.1 0.4
Grade tensile strength Mpa yield strength Mpa elongation
Grade1 240 138 24

4. Titanium rod application:

Gr1 titanium bars can be used in environments up to 400°C and offer good resistance to general corrosion, pitting, and crevice corrosion. They can be easily machined, forged, or welded using common titanium fabrication techniques. These bars are available in various sizes and lengths, making them suitable for various applications, including bolts, fasteners, rivets, bicycle frames, and more.

We provide titanium rods for various industries. The most common applications of this material include aviation, the petrochemical industry, the construction of water treatment plants, power generation facilities, and offshore vehicles.

Detail Shows

titanium rod
6mm titanium rod

5. Permissible tolerance for Titanium Bars-Hot-Rolled Round and Square bars

Specified Size, in. (mm) Size Variations,
in. (mm)
Out-of-Round A or Out-of-Square, B in. (mm)
1 ⁄ 4 to 5 ⁄ 16 (6.35 to 7.94), incl ±0.005 (0.13) 0.008 (0.20)
5 ⁄ 16 to 7 ⁄ 16 (7.94 to 11.11), incl ±0.006 (0.15) 0.009 (0.23)
7 ⁄ 16 to 5 ⁄ 8 (11.11 to 15.88), incl ±0.007 (0.18) 0.010 (0.25)
5 ⁄ 8 to 7 ⁄ 8 (15.88 to 22.22), incl ±.008 (0.20) 0.012 (0.30)
7 ⁄ 8 to 1 (22.22 to 25.40), incl ±0.009 (0.23) 0.013 (0.33)
Over 1 to 1 1 ⁄ 8 (25.40 to 28.58), incl ±0.010 (0.25) 0.015 (0.38)
Over 1 1 ⁄ 8 to 1 1 ⁄ 4 (28.58 to 31.75), incl ±0.011 (0.28) 0.016 (0.41)
Over 1 1 ⁄ 4 to 1 3 ⁄ 8 (31.75 to 34.92), incl ±0.012 (0.30) 0.018 (0.46)
Over 1 3 ⁄ 8 to 1 1 ⁄ 2 (34.92 to 38.10), incl ±0.014 (0.36) 0.021 (0.53)
Over 1 1 ⁄ 2 to 2 (38.10 to 50.80), incl ± 6 1 ⁄ 64 (0.40) 0.023 (0.58)
Over 2 to 2 1 ⁄ 2 (50.80 to 63.50), incl + 1 ⁄ 32 , − 0 (0.79) 0.023 (0.58)
Over 2 1 ⁄ 2 to 3 1 ⁄ 2 (63.50 to 88.90), incl + 3 ⁄ 64 , − 0 (1.19) 0.035 (0.89)
Over 3 1 ⁄ 2 to 4 1 ⁄ 2 (88.90 to 114.30), incl + 1 ⁄ 16 , − 0 (1.59) 0.046 (1.17)
FAQ

Q: 1. What grades of pure titanium bars are there?

A: Common grades of pure titanium bars include: Gr1, Gr2, Gr3, Gr4, etc. Among them, the Gr1 titanium bar is the softest and has the highest purity, and so on.

Q: 2. What are the implementation standards of pure titanium bars?

A: The common implementation standards of Gr1 titanium bar and Gr2~Gr4 titanium bar are ASTMB348, ASTMF67, etc. German standards, Russian standards, and French standards can be customized according to requirements.

Q: 3. What is the purity of the Gr1 titanium bar?

A: The purity of the Gr1 titanium bar can reach more than 99.7%, and higher purity can be customized according to requirements.

Q: 4. Is the Gr1 titanium bar in stock?

A: Some specifications of the Gr1 titanium bar are in stock, and all specifications of the Gr2 and Gr5 titanium bars are in stock.

Q: 5. Can the Gr1 titanium bar be cut in half?

A: Gr1 titanium bar can be cut to length according to customer requirements, and can be sent by express, air, or sea.

Contact information:

Tel: +86-0917- 3664600

Whatsapp: +8618791798690

Email: sales@tmsalloy.com
tina@tmsalloy.com

Hot Tags: high purity astmb348 gr1 titanium bar, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ASTM F136 Titanium Bar Ti-6al-4V, Precision Titanium Round Bar Rod Ti-6Al-4V ELI, Ti6al4V Eli Titanium Bar, 10mm TA6V Grade 5 Titanium Rod, Ti6al4v Grade 5 3 7165 Titanium Hollow Bar ASTMB348, Precision Titanium Round Bar Rod Ti 6Al 4V ELI

Send Inquiry

(0/10)

clearall