Ti6al4v alloy GOST23755 BT6 Titanium Plate

Ti6al4v alloy GOST23755 BT6 Titanium Plate

BT6 Titanium alloy sheet
1.Ti-6AL-4V TA6V titanium alloy
2. Thick 0.5~200mm
3. 1000x2000mm or fixed wide and length
4. ΓOCT23755-87 ΓOCT22178-90 DIN17860-1990
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of ti6al4v alloy gost23755 bt6 titanium plate in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

Products Introduction

1. One of the most popular titanium alloy plates, the BT6 titanium plate is a Russia-grade titanium metal sheet that has high strength and good corrosion resistance.

2. Titanium alloy sheet BT6 available size and standards

OD: 0.5~200mm or the customer's size

Standards: ΓOCT23755-87 ΓOCT22178-90 DIN17860-1990

3. Titanium alloy sheet BT6 properties

In comparison to Grade 5 titanium alloy, it has additional Zr and Si components, as well as the high tensile strength Al and V element, BT6 (Al 5.36.8, V 3.55.3).

BT6 (VT6) titanium sheet
titanium alloy sheet BT6

4. The titanium plate BT6(VT6) chemical 's make-up

GradeChemical composition (mass fraction) (%) is not greater than (except for the specified range value)

TiAlCrMoSnMnVFeSiZrCNHOthe sum of other elements
VT6base5.3~6.83.5-5.30.60.150.30.10.050.0150.20.3
BT1-0base0.3~0.70.250.10.070.040.010.20.3
Russian titanium and titanium alloy grades and chemical composition




GradeChemical composition (mass fraction) (%) is not greater than (except for the specified range value)
TiAlCrMoSnMnVFeSiZrCNHOthe sum of other elements
BT1-00base0.150.080.050.040.0080.10.1
BT1-0base0.250.10.070.040.010.20.3
BT1-2base1.50.150.10.150.010.30.3
OT4-0base0.4~1.40.5~1.30.30.120.30.10.050.0120.150.3
OT4-1base1.5~2.50.7~2.00.30.120.30.10.050.0120.150.3
OT4base3.5~5.00.8~2.00.30.120.30.10.050.0120.150.3
BT5base4.5~6.20.80.30.120.30.10.050.0150.20.3
BT5-1base4.3~6.02.0~3.00.30.120.30.10.050.0150.150.3
BT6base5.3~6.80.60.10.30.10.050.0150.20.3
BT6Cbase5.3~6.50.250.150.30.10.040.0150.150.3
BT3-1base5.5~7.00.8~2.02.0~3.00.2~0.70.15~0.040.50.10.050.0150.150.3
BT8base5.8~7.02.8~3.80.30.2~0.40.50.10.050.0150.150.3
BT9base5.8~7.02.8~3.80.250.2~0.351.0~2.00.10.050.0150.150.3
BT14base3.5~6.32.5~3.80.250.150.30.10.050.0150.150.3
BT20base5.5~7.00.5~2.00.250.151.5~2.50.10.050.0150.150.3
BT22base4.4~5.70.5~1.54.0~5.50.5~1.50.150.30.10.050.0150.180.3
ПT-7Mbase1.8~2.50.250.122.0~3.00.10.040.0060.150.3
ПT-3Bbase3.5~5.00.250.120.30.10.0400.150.3
AT3base2.0~3.50.2~0.50.2~0.50.2~0.40.10.050.0080.150.3

5. What are the uses of BT6 titanium plates?

BT6 alloy (Ti-6Al-4Vl has found a wide application in the fabrication of titanium welded structures).

6. Our benefits

Our primary goal is to be a reputable supplier of titanium metal sheets and BT6 Titanium plates at reasonable costs. We are a Titanium Alloy Sheet BT6 Supplier in Baoji and perfect after-sale service to our customers. We follow the path of professional growth and dominate the industry with our cutting-edge technological advancements and superior product caliber.

7. Package and delivery

Standards export package: wooden case package or wooden pallet packaging

10kg or below are carton or woven bag packaging

delivery and package baoji fairy titanium tmsalloy.com

Hot Tags: ti6al4v alloy gost23755 bt6 titanium plate, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ASTMB265 Ti 0 2Pd Gr11 Titanium Plate, CT23755 87 Ti 5AL 2 5Sn Gr6 BT5 1 Titanium Plate, ASTMB265 3 7105 UNS R53400 Gr12 Titanium Sheet, Sintered Porous Plate 1Mm Thickness Titanium Porous Metal Sintered Plate, ASTMB265 Ti 0 05Pd Gr16 Titanium Sheet, ASTMB265 Ti 0 05Pd Gr17 Titanium Plate

Send Inquiry

(0/10)

clearall