1. Titanium clad copper bar is a metal composite titanium material coated with a certain thickness (generally 1.0~1.2mm) titanium layer on the circumference of the copper rod.

2. Products information

Material: Gr1,Gr2.etc

cover thickness:0.5-3 mm

primary thickness: above3.5mm

width:1500-2600mm

Titanium clad copper bar is divided according to its cross-sectional geometry, mainly round, flat, square, rectangular, drum shape, and so on.

Titanium copper bar anode/ composite bar/ rod specifications:

1. Forming: Round, Square, Rectangle, Hex, Octagonal

2. Ti+Cu; Zi+Cu

Section shape
 
Section size(mm) cladding material Substrate material
layer thickness material  
square Side length(10-40) 1.0-2.5

Ti,Zr,Ni,

Stainless steel

T1,T2, TU1,TU2,AL, Stainless steel, etc
rectangle

Side length(20-160)

side width(10-30)

1.0-2.5
drum

Side length

(25,27,29,32,34)*14

1.0-2.5
round Dia(8-50) 1.0-2.5
wire material Dia(2.0-8.0) 1.0-2.5

3. This composite titanium material combines the excellent conductivity of copper with the outstanding corrosion resistance of titanium. It can be used as a conductor carrying large currents under strong corrosive working conditions while ensuring the uniformity of current density. , Eliminates the electrolyte pollution caused by the corrosion of the copper conductor. Therefore, titanium clad copper bar has become the main part of the production of metal anode electrolyzers.

Detail Shows

titanium clad copper bar

Titanium copper bar

Ti-Cu clad bar

Ti-Cu clad bar

4. Ti Clad Copper bar is manufactured by bonding metallurgical C.P.Titanium to an OFHC (Oxygen-free high conductivity) Copper core, they have excellent conductivity, high ductility, and weldability.

5. High-quality titanium Copper Bar for metal anode application:

Titanium-clad copper bar is mainly used in electrolysis, electroplating, hydrometallurgy, and metal anode electrolyzers under strong corrosion conditions. On the one hand, it has the excellent conductivity of the intermediate material copper, on the other hand, it owns the corrosion resistance of the coating material, which is a high-quality electrode material.

Titanium Clad Copper Weld Bus Bar

Titanium Clad Copper Bus Bar

titanium clad copper rod

Titanium-clad copper rod

Titanium-clad copper has excellent conductivity, full ductility for forming and shaping, good weldability for connection, cover, and joint, high corrosion resistance, and long service life of titanium layer.

Other applications are also like petroleum chemical industry, energy engineering, ocean engineering, surface treatment, and electrode manufacturing.

6. FAQ

Q: 1. How big can the titanium-copper bar be made?

A: The minimum size of round titanium-copper composite rods can be 12mm; the rectangle titanium-clad copper bar min size can be 30x6mm.

Q: 2. Is there a minimum order quantity for titanium-clad copper bars?

A: The minimum order quantity for titanium clad copper bars is 1~2 pieces, non-standard size or customized MOQ50KG

Q: 3. Application of titanium-clad copper rods in electrolytic cells

A: As a place for electrochemical reactions, electrolyzers need to pass electric current to promote the reaction.
Features of titanium-clad copper bar: Fairy titanium-clad copper rod can not only ensure the original conductive properties of copper, but also use titanium covering to protect the copper body from corrosion, and greatly reduce the electroplating and electroplating liquid pollution. It has good electrical conductivity and can effectively transmit current and improve the efficiency and reaction rate of electrolytic cells.

Contact us 

Tel: +86-0917- 3664600

Whatsapp: +8618791798690

Email: sales@tmsalloy.com
tina@tmsalloy.com

Hot Tags: titanium clad copper bar, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Titanium Stainless Steel Clad Plate, TI-SS Clad Plate, Gr.1 Titanium Carbon Steel Clad Tubesheet, Titanium Clad Steel tube plate, Titanium stainless Clad Steel Plates, Titanium Clad Tube Sheet Plates

Send Inquiry

(0/10)

clearall