Grade2 Eccentric Titanium Reducer

Grade2 Eccentric Titanium Reducer

3" titanium reducer
Concentric titanium reducer
Eccentric titanium reducer
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of grade2 eccentric titanium reducer in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

Products Introduction

1. Metal pipe fittings for tube connections include titanium reducers. The small and large heads' centers are located on the centerline of the tube, which is known as a concentric reducer. If not, it is referred to as an eccentric reducer.

2. Basic Information

Grade 2 Titanium Concentric Reducer Data Sheets Schedule 10S

Nominal Pipe SizeOutside Diameter

Length

Schedule 10S Light N.P.S.
Large End
Small EndLarge EndSmall End

Approx. Wt. in Lbs./Kgs

Inside DiameterWall Thick.Inside DiameterWall Thick.
ininmminmminmminmminmminmminmmlbkg
3/4 x 1/21.0526.670.8421.342.0050.800.8822.450.082.110.6717.120.082.110.130.06
1 x 1/21.3233.400.8421.342.0050.801.1027.860.112.770.6717.120.082.110.150.07
1 x 3/41.3233.401.0526.672.0050.801.1027.860.112.770.8822.450.082.110.170.08
1-1/2 x 1/21.9048.260.8421.342.5063.501.6842.720.112.770.6717.120.082.110.210.10
1-1/2 x 3/41.9048.261.0526.672.5063.501.6842.720.112.770.8822.450.082.110.220.10
1-1/2 x 11.9048.261.3233.402.5063.501.6842.720.112.771.1027.860.112.770.250.11
2 x 3/42.3860.331.0526.673.0076.202.1654.790.112.770.8822.450.082.110.320.15
2 x 12.3860.331.3233.403.0076.202.1654.790.112.771.1027.860.112.770.350.16
2 x 1-1/22.3860.331.9048.263.0076.202.1654.790.112.771.6842.720.112.770.390.18
3 x 13.5088.901.3233.403.5088.903.2682.800.123.051.1027.860.112.770.590.27
3 x 23.5088.902.3860.333.5088.903.2682.800.123.052.1654.790.112.770.690.31
4 x 24.50114.302.3860.334.00101.604.26108.200.123.052.1654.790.112.770.990.45
4 x 34.50114.303.5088.904.00101.604.26108.200.123.053.2682.800.123.051.100.50
6 x 36.63168.283.5088.905.50139.706.36161.470.133.403.2682.800.123.052.291.04
6 x 46.63168.284.50114.305.50139.706.36161.470.133.404.26108.200.123.052.471.12
8 x 48.63219.084.50114.306.00152.408.33211.560.153.764.26108.200.123.053.801.72
8 x 68.63219.086.63168.286.00152.408.33211.560.153.766.36161.470.133.404.031.83
10 x 610.75273.056.63168.287.00177.8010.42264.670.174.196.36161.470.133.406.312.86
10 x 810.75273.056.63168.287.00177.8010.42264.670.174.198.33211.560.153.766.552.97
12 x 612.75323.856.63168.288.00203.2012.39314.710.184.576.36161.470.133.409.374.25
12 x 812.75323.858.63219.088.00203.2012.39314.710.184.578.33211.560.153.769.674.39
12 x 1012.75323.8510.75273.058.00203.2012.39314.710.184.5710.42264.670.174.1910.004.54

When there is a change in diameter, titanium concentric reducers are used to connect pipes or tubes in parts.

Dimensional tolerances for titanium reducers are compliant with ASME B16.9. Pipe fittings must adhere to ASME B36.19M specifications 10s and 40s for wall thickness.

Detail Shows

ECCENTRIC titanium reducer

Eccentric titanium reducer

Concentric titanium reducer

Concentric titanium reducer

3. Among the industries where titanium reducers are used are of oil and gas pipeline engineering, natural gas pipeline engineering, chemical plants, power plants, shipyards, pharmacies, dairy products, alcoholic beverages, water conservation, etc.

titanium reducer pipe fittings (2)

Hot Tags: grade2 eccentric titanium reducer, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ASME B16 9 90 Degree Gr2 Gr12 Titanium Elbows, ANSI/ASME B16.9 Equal Tee Titanium, Grade2 Concentric Titanium Reducer, UNS R52400 Titanium Grade 7 Concentric Reducers, ASTM B363 Grade 2 Titanium Lap Joint Stub Ends, Grade 2 Titanium Straight Tee Pipe Tee Fittings

Send Inquiry

(0/10)