1. Nickel tape is a kind of metal strip made of pure nickel and nickel alloy, Ni200, Ni201, and other alloy grades, it is widely used for battery welding, battery connection,
2. Basic information
Specification of nickel strip: (thickness * width * length / mm): 0.03-1.20 * 2-150 * ≥ 3000
Status: soft (m), semi-hard (Y2), hard (Y)
Density 8.9 g / cm3,
melting point 1455 ℃
Process: hot rolling or cold rolling
3. Nickel strips feature excellent heat-resistant concentrated alkali solution corrosion, and excellent corrosion resistance to alkaline and neutral solution media of carbonate, nitrate, oxide, and acetate.
Detail Shows


4. Pure nickel strips have excellent corrosion resistance, magnetostriction and magnetism, low gas volume, and low vapor pressure. Nickel tape also has good luster, ductility, and weldability. High-purity nickel strip has good corrosion resistance under the conditions of low temperature and high concentration of alkaline and chloride ions. Pure nickel strip for high magnification power tool battery pack, notebook battery, and aircraft model battery combination. Nickel stripe has a good spot welding function, high tensile tension, convenient operation, and low resistivity. It can pass through more than 50A current. It is a high-quality choice for power battery pack combinations. Nickel strip is mainly used for manufacturing nickel-hydrogen batteries, lithium batteries, combined battery and electric switching tools, communication information, special lamp, and other industries.
5. Surface quality:
(1) The nickel tape surface shall be smooth and clean without wind layer, crack, bubble, pricking, crimping, or inclusion.
(2) Slight local scratches, spots, pits, inserts, roller marks, and other defects that do not make the strip thickness exceed the allowable deviation are allowed, and slight oxidation color, darkening, and slight local oil stains are not used as the basis for scrapping.
(3) Both sides of the strip shall be cut flush without burr, crack, or crimping.
(4) The strip shall be straight, but slight waves are allowed; The side curvature of the strip shall not be greater than 3mm per meter.