Nickel Wire 0.025mm

Nickel Wire 0.025mm

nickel wire 0.025mm
nickel 200 wire
nickel wire price
pure nickel wire
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of nickel wire 0.025mm in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

Products Introduction

1. Nickel wire 0.025mm is a metal wire made of nickel, which is a sliver white wire on a spool.

2. Basic Information

Grade: Nickel 200, Nickel 201 (UNS N02200, UNS N02201)

Standards: ASTM B166

Diameters: 0.025, 0.19, 0.2, 0.3, 0.4, 0.5, 0.6mm etc.

Melting point 1446 degrees Celsius

Density 8.89 g/cm3

Nickel 200 is pure nickel with good performance and outstanding alkali corrosion resistance (like sodium hydroxide). It also has good mechanical strength, corrosion resistance, and high heat resistance.

Detail Shows

nickel 200 wire

nickel 200 wire

pure nickel wire

pure nickel wire

3. Nickel wire 0.025mm applications: wire-wound resistors, electric heaters, heating plates, electric heating coils, shunts for small household appliances (electric kettles, coffee pots, toasters, etc.), precision resistance components, high-temperature-resistant wires and cables for wire-wound resistors, lead wire at the connection of heating element, high-temperature nickel plating, ceramic heating piece lead, temperature sensing wire, temperature measurement wire.

4. Nickel wire 0.025mm chemical elements according to ASTMB160

Chemical elementsNickel minCu maxFe maxMn maxC maxSi maxS max
Nickel(UNSN02200)990.250.40.350.150.350.01
Low-C nickel(UNS N02201)990.250.40.350.020.350.01

Hot Tags: nickel wire 0.025mm, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Shape Memory Nitinol Wire, Nickel 201 Wire, 99 6 Purity Nickel 200 Wire, nitinol memory