Titanium standard- GB-ASTM-JIS-DIN-OCT

Oct 10, 2021

Titanium and titanium alloy standards

1、 Chinese standards

1. Chinese national standards

GB / t2524-2007 titanium sponge

GB / t3620-2007 titanium and titanium alloy grades and chemical compositions

GB / t15073-1994 grades and chemical compositions of cast titanium and titanium alloys

GB / t3621-2007 titanium and titanium alloy sheet

GB/T14845-1993 Titanium plate for plate heat exchanger

GB / t3622-1999 titanium and titanium alloy strip and foil

GB / t3623-2007 titanium and titanium alloy wire

GB / t3624-2007 titanium and titanium alloy pipes

GB / t3625-2007 titanium and titanium alloy tubes for heat exchanger and condenser

GB / t2965-2007 titanium and titanium alloy bars

GB/T16598-1996 Titanium and titanium alloy cakes and rings

GB/T8546-1987 Titanium stainless steel clad plate

GB/T8547-1987 Titanium steel composite plate

GB/T6614-1994 Titanium and titanium alloy castings

GB / t5168-1985 test method for macrostructure of two phase titanium alloy

GB / t6611-2008 terminology of titanium and titanium alloys

GB / t8755-2008 metallographic Atlas of terms for titanium and titanium alloys

T12769-2003 titanium composite rod

GB / t13810-2007 titanium and titanium alloy processing materials for surgical implants

GB / t12417-1990 general specification for surgical metal implants

GB/T4698.1-4698.25-1996 Methods for chemical analysis of sponge titanium, titanium and titanium alloys

GB / t5193-2007 ultrasonic testing method for titanium and titanium alloy processed products

GB/T12969.1-1991  Ultrasonic testing method for titanium and titanium alloy pipes

GB/T13149-1991 Eddy current testing method for titanium and titanium alloy tubes

GB / t13149-1991 titanium and titanium alloy meet the welding technical requirements of steel plate

Sintered titanium filter elements and materials

GB / t8180-2007 packaging, marking, transportation and storage of titanium and titanium alloy processed products

TA7 titanium alloy plates for important applications

TC4 titanium alloy plates for important applications (GB / t6613-1986)

Welding specification for TA5 titanium alloy (GB / t1216-1992)

2. Chinese national military standards

Gjb2218-1994 specification for titanium and titanium alloy bars and forgings for aviation

Specification for titanium and titanium alloy bars (wires) for fasteners (gjb2219-1994)

Gjb2220-1994 specification for titanium alloy cake and ring blank for Aeroengine

Gjb2505-1995 specification for titanium and titanium alloy plate and strip for aviation

Gjb2744-1996 specification for titanium and titanium alloy bars, free forging and die forgings for aviation

Gjb2896-1996 specification for titanium and titanium alloy investment castings

Specification for TC4 titanium alloy sheet for superplastic forming (gjb2921-1997)

Gjb3763a-2004 heat treatment of titanium and titanium alloys

Gjb391-1987 TC4 titanium alloy for aerospace industry

Gjb493-1988 TC4 titanium alloy bars for Aeroengine Blades

Gjb494-1988 TC11 titanium alloy bars for Aeroengine Blades

Gjb495-1988 ta7-d titanium alloy bar for ultra low temperature

Ta5-a titanium alloy forgings for submarine gjb943-1900

Gjb944-1900 ta5-a titanium alloy plate

Gjb1169-1991 specification for titanium alloy rings for aerospace applications

Technical specification for tjb1205-1991 tb2-1 titanium alloy rivets

Specification for TC4 titanium alloy bars for aircraft structures (gjb1538-1992)

2、 American Standard

1. ASTM standards

Astmb229-2001 titanium sponge

Astmb265-2005 titanium and titanium alloy strip, sheet and plate

ASTM b337-1995 titanium and titanium alloy seamless pipe and welded pipe (has been replaced by b861-2002 titanium and titanium alloy seamless pipe, b862-2002 titanium and titanium alloy welded pipe)

ASTM b338-2005a seamless and welded tubes for titanium and titanium alloy condensers and heat exchangers

ASTM b348-2005 titanium and titanium alloy bars and billets

ASTM b363-2004 non alloy titanium and titanium alloy seamless and welded pipe fittings

ASTM b367-2004 titanium and titanium alloy castings

ASTM b861-2002 titanium and titanium alloy seamless pipe

ASTM b862-2002 titanium and titanium alloy welded pipe

ASTM b381-2005 titanium and titanium alloy forgings

ASTM f67-2000 pure titanium for surgical implants

ASTM f136-2002a Ti-6Al-4V Eli processed materials for surgical implants

ASTM f620-2002 α + β phase titanium alloy forgings for surgical implants

Astmf1108-2002 Ti-6Al-4V castings for surgical implants

Astmf1295-2001 Ti-6Al-7Nb processed materials for surgical implants

Astmf1341-1999 pure titanium wire

ASTM f1472-2002a Ti-6Al-4V processed materials for surgical implants

Astmf1713-1996 ti-13nb-13zr processed materials for surgical implants

Astmf1813-2001 ti-12mo-6zr-2fe processing material for surgical implants

ASTM f2063-2000 shape memory alloy processing materials for medical devices and surgical implants

2. American Society of Mechanical Engineers standards

ASME Section VIII: Section I pressure vessels (basic rules)

American aerospace materials technical standard

AMS 4900-2001 titanium sheet, strip and plate (annealed) (380MPa)

Ams4901-2002 titanium sheet, strip and plate (annealed) (485mpa)

Ams4902-2001 titanium sheet, strip and plate (annealed) (275mpa)

Ams4907-2001 ultra low gap element grade Ti-6Al-4V alloy sheet, strip and plate (annealed state)

Ams4910-2003 ti-5al-2.5sn alloy sheet, strip and plate (annealed state)

Ams4911-2003 Ti-6Al-4V sheet, strip and plate (annealed condition)

AMS4921-2004 Titanium bars, forgings and rings (annealed) (485mpa)

Ams4924-2002 ultra low gap element grade ti-5al-2.5sn alloy bars, forgings and rings (annealed condition)

Ams4926-2001 ti-5al-2.5sn rods and rings (annealed) (760mpa)

Ams4928-2001 Ti-6Al-4V alloy bars, forgings and rings (annealed) (825mpa)

Ams4941-2003 titanium welded pipe

Ams4942-2001 seamless titanium tube (annealed) (275mpa)

Ams4930-2001 ultra low gap element grade Ti-6Al-4V alloy bars, forgings and rings (annealed condition)

Ams4951-2003 industrial pure titanium welding wire

Ams4954-2003 Ti-6Al-4V alloy welding wire

Ams4965-2002 Ti-6Al-4V alloy bars, forgings and rings (solution and stabilization treatment)

Ams4966-2003 ti-5al-2.5sn forgings

Ams4967-2001 heat treatable Ti-6Al-4V alloy bars, forgings and rings (annealed condition)

Asm4972-2003 ti-8al-1mo-1v alloy bars and rings (solution and stabilization treatment)

Asm4973-2002 ti-8al-1mo-1v titanium alloy forgings (solution and stabilization treatment)

Asm4975-2003 ti-6al-2sn-4zr-2mo alloy bars and rings (solution and stabilization treatment)

Asm4983-2002 ti-10v-2f-3al forging (solution treatment and aging)

Asm4985-2003 Ti-6Al-4V alloy forgings cast by paraffin or graphite tamping method

Asm4991-2002 Ti-6Al-4V alloy precision forging (annealed state)

Approval and control of asm2380-2003 high quality titanium alloy

3. US military standards

Mil-t-9046-1999 titanium and titanium alloy sheet, strip and plate

Mil-t-9047-2005 titanium and titanium alloy bars and forgings

Mil-r-81588-1986 titanium and titanium alloy rods and wires

Mil-f-83142-2000 titanium and titanium alloy forgings (high quality)

Mil-t-46077 titanium alloy weldable armor plate

Mil-t-13405 titanium powder

Mil-t-46035-1989 high strength titanium alloy and deformation material

Mil-t-81556-1996 round bars, bars and extrusions of titanium and titanium alloys

Heat treatment of mil-t-81200 titanium and titanium alloy

3、 British Standard

Bs2ta1: 1974 sheet and strip of industrial pure titanium (tensile strength 290-420mpa)

Bs2ta2: 1973 industrial pure titanium sheet and strip (tensile strength 390-540mpa)

BS 2ta3:1973 industrial pure titanium bars and profiles for machining (tensile strength 390-540mpa)

BS 2ta4:1973 forging stock of industrial pure titanium (tensile strength 390-540mpa)

BS 2ta5:1973 forging stock of industrial pure titanium (tensile strength 390-540mpa)

Bs2ta6: 1973 industrial pure titanium sheet and strip (tensile strength 570-730mpa)

Bs2ta7: 1973 industrial pure titanium bars and profiles for machining (tensile strength 540-740mpa)

Bs2ta8: 1973 forged blanks of industrial pure titanium (tensile strength 540-740mpa)

Bs2ta9:1973 industrial pure titanium forgings (tensile strength 540-740mpa)

Bs2ta10:1974 titanium aluminum vanadium alloy sheet and strip (tensile strength 960-1270mpa)

Bs2ta11:1974 titanium aluminum vanadium alloy bars and sections for machining (tensile strength 900-1160mpa)

BS 2ta12:1974 Ti Al V alloy forging stock (tensile strength 900-1160mpa)

Bs2ta13:1974 titanium aluminum vanadium alloy forgings (tensile strength 900-1160mpa)

Bs2ta21:1973 titanium copper alloy sheet and strip (tensile strength 540-770mpa)

BS 2ta22:1973 titanium copper alloy bars and sections for machining (tensile strength 540-770mpa)

BS 2ta23:1973 titanium copper alloy forging stock (tensile strength 540-770mpa)

Bs2ta24:1973 titanium copper alloy forgings (tensile strength 540-770mpa)

BS 2ta28:1974 Ti Al V alloy forging stock and wire (tensile strength 1100-1300mpa)

Bsta38:1993 titanium aluminum molybdenum tin silicon carbon alloy bars for machining (tensile strength 1250-1420mpa)

Bsta39:1993 forging stock of Ti Al Mo Sn Si C alloy (tensile strength 1250-1420mpa)

Bsta40:1993 titanium aluminum molybdenum tin silicon carbon alloy bars for machining (tensile strength 1250-1375mpa)

Bsta41:1993 forging stock of Ti Al Mo Sn Si C alloy (tensile strength 1250-1375mpa)

Bsta42:1993 titanium aluminum molybdenum tin silicon carbon alloy forgings (tensile strength 1250-1375mpa)

Bsta45:1993 titanium aluminum molybdenum tin silicon alloy bars and sections for machining (tensile strength 1100-1280mpa)

Bsta46:1993 titanium aluminum molybdenum tin silicon alloy bars and sections for machining (tensile strength 1050-1220mpa)

Bsta47:1993 forging stock of Ti Al Mo Sn Si alloy (tensile strength 1050-1220mpa)

Bsta48:1993 forging stock of Ti Al Mo Sn Si alloy (tensile strength 1050-1220mpa)

Bsta49:1993 titanium aluminum molybdenum tin silicon alloy bars and sections for machining (tensile strength 1000-1200mpa)

Bsta50:1993 forging stock of Ti Al Mo Sn Si alloy (tensile strength 1000-1200mpa)

Bsta51:1993 titanium aluminum molybdenum tin silicon alloy forgings (tensile strength 1000-1200mpa)

Bsta52:1993 titanium copper alloy sheet and strip (tensile strength 690-920mpa)

Bsta66:1993 thick plate of Ti Al V alloy (tensile strength 895-1150mpa)

Bsta57:1993 titanium aluminum molybdenum tin silicon thick plate (tensile strength 1030-1220mpa)

Bsta58:1993 thick plate of titanium copper alloy (tensile strength 520-640mpa)

Inspection and experimental methods of bsta100:1973 deformed titanium and titanium alloys

Bs5500:1997 flameless fusion welding pressure vessel

Lining and chemical equipment of cp3003 pressure vessel

4、 Russian standard

Γ oct17746-79 titanium sponge

Γ oct19807-91 wrought titanium and titanium alloy grades

Γ oct22178-90 titanium and titanium alloy sheet

Γ oct23755-87 titanium and titanium alloy thick plate

Γ oct21945-82 hot rolled seamless titanium tube

Γ oct22897-86 cold rolled seamless titanium tube

Γ oct24890-81 welded titanium pipe

Γ oct26492-85 titanium and titanium alloy rolling bar

Specification of Γ oct27265-87 titanium and titanium alloy filler wire

5、 Japanese standard

Jish2151-1983 sponge

Jish4600-1993 titanium and titanium alloy plate and strip

Jish4630-1994 titanium and titanium alloy seamless pipe

Jish4631-1994 titanium and titanium alloy heat exchanger tubes

Welding of titanium alloy ji4635

Jish4650-2000 titanium and titanium alloy rod

Jish4657-1998 titanium and titanium alloy forgings

Jish4670-1993 titanium and titanium alloy wire

Jis7505 titanium casting

6、 German standard

Chemical composition of din17850-1990 industrial pure titanium for pressure working

Chemical composition of din17851-1990 titanium alloy pressure working materials

Din17860-1990 titanium and titanium alloy plate and strip

Din17861-1990 titanium and titanium alloy seamless pipe

Din17862-1990 titanium and titanium alloy bars

Din17863-1973 titanium and titanium alloy wire

Din17864-1993 titanium and titanium alloy forgings

Din17865-1990 cast titanium

Din17866-1990 titanium and titanium alloy welded pipe

Chemical composition and technical conditions of titanium and titanium palladium alloy filling materials

Din1737t2-1988 titanium and titanium palladium alloy filler materials -- test block, specimen, mechanical and technological properties

DIN931 external hexagon bolt half thread

DIN933 external hexagon bolt full thread

DIN931 outer hexagon nut

DIN125 ordinary gasket

DIN127 spring washer

7、 French Standard

Nfl21-1101975 pure titanium T40 forging bar blank

Nfl21-2701981 TA6V rivet wire rod

Nfl16014 for forging

Nfl14-6021984 TA6V forgings

Nfl14-6031984 TA6V bar blank for forging

Nfl14-6041984 TA6V forging

Nfl14-6111984 ta6vzr5d bar blank

Nfl14-6121984 ta6vzr5d forging

8、 ISO international standard (titanium standard for surgical implants)

Iso5832-2-1999 pure titanium

ISO 5832-3-1996 Ti-6Al-4V processed timber

ISO 5832-11-1994 Ti-6Al-7Nb processed timber