Medical Titanium Bar --The metal bone implanted in the body

Mar 31, 2022

Titanium and titanium alloy materials are widely used in the nuclear industry, chemical and petrochemical industry, aerospace, sporting goods, dentistry, and medical restoration. As a professional supplier,we can provide you with Medical Titanium Bar at a competitive price, Titanium alloy materials are also selected as the best materials to replace or repair failed hard tissues (structural biomedical applications).

Pure titanium has good corrosion resistance, while its biocompatibility and comprehensive mechanical properties are poor, its strength is relatively low and its production cost is also very expensive. The emergence of titanium alloy can be well replaced.

Titanium alloy can better meet the performance requirements than stainless steel, industrial pure (CP) Nb, Cr Co alloy, CP TA, and other medical application materials. Due to the formation of an oxide layer on its surface, titanium alloy has excellent corrosion resistance and low elastic modulus.

Medical Titanium Bar is not only non-toxic, lightweight, high specific strength, excellent biocompatibility, and corrosion resistance, but also can be used as implants implanted in the human body. It is an ideal medical metal material. Moreover, titanium is abundant in the earth's crust and has the potential for further development. It is an ideal biomedical engineering material with broad application prospects.

Medical Titanium Bar

At present, pure titanium (TA1, TA2; TA1 is titanium with a purity greater than 99.6%, and its purity less than 99.6 is TA2) and Ti-6Al-4V、Ti-5Al-2.5Fe and Ti-6Al-7Nb alloys are widely used in the medical field, but they are new β Because of its better biocompatibility and mechanical compatibility, type-I titanium alloy has become the research hotspot of new medical titanium alloy and the most potential technology in the field of medical implants.

In the future, the production technology of titanium alloy will develop towards low modulus and high strength. From the development trend, β Type titanium alloy will become the direction of future development and the "leader" of the medical titanium alloy market.

Now, Chinese researchers have synthesized dental Ti Zr alloy with reference to the mechanical properties of CO Cr alloy and type IV alloy commonly used in clinics, which is expected to become a new titanium alloy for oral repair. In addition, our country has also designed TAMZ type (Ti-Al Mo Zr, etc.) medical alloy, which has better compatibility and low price, and is suitable for making dental stents and snaps rings.

I believe that with the development of science and technology, China's research on titanium alloy will be more in-depth and thorough.