On January 2, 2024, Gr1 titanium sheet 1.5mm was shipped to customers, for a total of 4.2 tons. Gr1 titanium sheet is the purest and softest type of pure titanium and can be used for bending, stamping, and other corrosion-resistant chemical equipment workpieces.

How much is 1 kg of 1.5 titanium sheet?
The density of titanium is 4.51g/cm3, and the unit weight of 1.5 titanium sheets per square meter is 6.76kg (theoretical weight). This means that the size of 1kg1.5 titanium sheet is 1/6.76=0.147M2. The higher the unit weight of the titanium sheet, the thicker the thickness.

What is the price of a 1.5-titanium sheet?
The price of a 1.5 titanium plate varies according to the brand, quantity, and size. Common specifications and sizes are 1000x2000, 1250x3000, 1500x3000mm, etc. Common brands are Gr1 Gr2 Gr3 Gr4 Gr5 Gr7 Gr9 Gr12, etc. The specific price varies according to the brand and quantity.
Is a 1.5-titanium sheet available?
Gr1 Gr2 Gr3 Gr4 Gr5 Gr7 Gr9 Gr12 1.5 titanium plate common specifications are available, such as 1000x2000, other sizes can be customized according to customer requirements.
In addition to the 1.5 titanium sheet, what are the thinner titanium sheets?
The thinnest titanium sheet, titanium coil can be 0.3x1000, 0.3x1200mm, thinner titanium foil, titanium strip can be about 0.025x100 wide.
In addition to titanium sheets, we can also produce titanium foils, titanium strips, titanium forgings, titanium flanges, etc. For more titanium sheet prices, please get in touch with our sales engineers.
Contact information:
Tel: +86-0917- 3664600
Whatsapp: +8618791798690