On January 12, 2025, Baoji Fairy Titanium industry Co., Ltd. sent EHA300x4 titanium dish head to customer. Titanium dish head refers to the component used to seal the end of the container to isolate the internal and external media, also known as the end cover. According to the shape of the surface of the titanium dish head, it can be divided into convex, conical, flat and combined shapes. Convex head refers to the head with a convex outer surface shape, such as hemispherical, elliptical, dish-shaped and spherical head without folding edge.
What are the advantages of titanium dish head?
1. Lightweight, high strength, and good pressure bearing: The density of titanium is about 4.5g/cm³, which is only 57% of steel, but its strength is very high, about 2 times the hardness of ordinary steel and about 6 times that of aluminum. Good pressure bearing capacity. This allows the titanium head to ensure greater pressure bearing capacity at a lower weight, with greater safety and reliability, and has significant advantages in the chemical, pharmaceutical and other fields.
2. Strong corrosion resistance: Titanium and its alloys have excellent chemical stability. Head products made of titanium materials can resist the corrosion of chemical substances such as acid, alkali and salt. It is widely used in the production of container heads.
3. Good heat resistance: Titanium material has excellent heat resistance and can maintain stable physical and chemical properties in high temperature environment. Titanium alloy still maintains good mechanical properties at around 300℃. Based on these advantages, it has unique advantages in high-temperature application scenarios such as aerospace and military industry.
4. Easy to process and shape: In addition, titanium material also has good processing performance, which can meet the processing requirements of various complex shapes and sizes. It is an indispensable sealing component in various high-end equipment, ensuring the normal operation and use of the equipment. convoy.