Titanium wire perfectly inherits the advantages of titanium and titanium alloy and has a series of excellent characteristics such as good corrosion resistance, high specific strength, nonmagnetic, high biocompatibility, low resistance to ultrasonic waves, and good shape memory function.

Titanium and titanium alloy wires are widely used in many fields such as aerospace, petrochemical, medical and health care, automobile, construction, sports, and leisure goods. Moreover, in recent years, due to its continuous development, its variety has become increasingly diverse, which provides more choices for its application in high-performance industrial products and consumer goods.
1. At present, more than 80% of titanium and titanium alloy wires are used as welding wires, such as the welding of various titanium equipment, welding pipes, repair welding of turbine discs and blades of aviation jet engines, welding of the gearbox, etc.
2. Due to its excellent corrosion resistance, titanium wire has been widely used in chemical, pharmaceutical, paper, and other industries. It can be woven into a mesh as a seawater filter, a purified water filter, a chemical filter, etc. 3. Titanium and titanium alloy wires are also used to manufacture fasteners, load-bearing components, springs, etc. because of their good comprehensive properties.
4. In the medical and health industry, due to their excellent biocompatibility, titanium, and titanium alloy wires are used to manufacture medical devices, implant crown fixation, skull fixation, etc.
5. Some titanium alloy wires with shape memory function, such as titanium nickel alloy wires, are used to make satellite antennas, shoulder pads for clothes, bras for women, glasses frames, etc.
6. In electroplating and water treatment industries, titanium and titanium alloy wires are used to manufacture various electrodes. With the development of the national economy, the demand for titanium and titanium alloy wires is increasing. At present, the supply is in short supply and the development potential is very large.