BS 2TA 10-1974Specification for the sheet of titanium-aluminum-vanadium alloy (tensile strength 960-1270 MPa)
BS 2TA 100-1973Procedure for inspection and testing of wrought titanium and titanium alloys
BS 2TA 11-1974Specification for bar and section for machining of titanium-aluminum-vanadium alloy (tensile strength 900-1160 MPa) (limiting ruling section 150 mm)
BS 2TA 12-1974Specification for forging stock of titanium-aluminum-vanadium alloy (tensile strength 900-1160 MPa) (limiting ruling section 150 mm)
BS 2TA 13-1974Specification for forgings of titanium-aluminum-vanadium alloy (tensile strength 900-1160 MPa) (limiting ruling section 150 mm)
BS 2TA 28-1974Specification for forging stock and wire of titanium-aluminum-vanadium alloy (tensile strength 1100-1300 MPa) (limiting ruling section 20 mm) (primarily intended for the manufacture of fasteners complying with the requirements of the 'A' series of British Standards)
BS 7252-3-1997Metallic materials for surgical implants - Specification for wrought titanium 6-aluminium 4-vanadium alloy
BS A 254, A 255, A 256, A 257, A 258, A 259-1976Specification - Hexagonal head titanium alloy bolts 160 000 lbf/inUP2 (1100 MPa)
BS A 266-1977Specification for 100 ° countersunk head titanium alloy bolts 160 000 lbf/in2 (1100 MPa) with Hi-torque speed drive recesses
BS A 352-2000Rivets, solid, in titanium or titanium alloy - Procurement specification
BS EN 2338-2001Aerospace series - Sheets, hot rolled in titanium and titanium alloys - Thickness 0,8 mm a 6 mm - Dimensions
BS EN 2339-2001Aerospace series - Sheets, cold-rolled in titanium and titanium alloys - Thickness 0,2 mm a 6 mm - Dimensions
BS EN 2545-1-1995Titanium and titanium alloy remelting stock and castings - Technical specification - General requirements
BS EN 2545-2-1995Titanium and titanium alloy remelting stock and castings - Technical specification - Remelting stock
BS EN 2545-3-1995Titanium and titanium alloy remelting stock and castings - Technical specification - Pre-production and production castings
BS EN 2617-2001Aerospace Series - Plates in titanium and titanium alloys - Thickness 6 mm a 100 mm - Dimensions
BS EN 2808-1997Anodizing of titanium and titanium alloys
BS EN 2858-1-1994Titanium and titanium alloys - Forging stock and forgings - Technical specifications - General requirements
BS EN 2858-2-1994Titanium and titanium alloys - Forging stock and forgings - Technical specification - Forging stock
BS EN 2858-3-1994Titanium and titanium alloys - Forging stock and forgings - Technical specifications - Pre-production and production forgings