Gr12 (Ti-0.3Mo-0.8Ni) titanium alloy is a corrosion-resistant titanium alloy. It is a near-α alloy developed to improve the crevice corrosion performance of pure titanium. The alloy contains 0.3% Mo and 0.8% Ni, which is not only strengthened It is an alloy and has good crevice corrosion performance to high temperature, low pH chloride, or weak reducing acid, and its corrosion resistance is significantly better than pure titanium and close to Gr7 alloy. Gr12 titanium alloy also has good process plasticity and welding properties and has been widely used in the chemical industry. Gr12 titanium plate is available in stock. The alloy can be used in an annealed state. Its main products include plates, bars, pipes, forgings, and wires.


There are two implementation standards for titanium plates, the national standards are GB/T3621-2007, GB/T13810-2007,
Gr12 titanium plate, the price of Gr12 titanium plate, the American standard is ASTM B265, ASTM F136, ASTM F67, AMS4928.
American label numbers: GR1, GR2, GR3, GR5, GR7, GR12
Russian label number: BT1-00, BT1-0, BT1-2, etc.
Domestic brands: TA0, TA2, TA3, TA5, TA6, TA7, TA9, TA10, TB2, TC1, TC2, TC3, TC4
Dimensions: T 0.5-5.0mm x W1000mm x L 2000-3500mm
T 6.0- 30mm x W1000-2500mm x L 3000-6000mm T 30- 80mm x W1000mm x L 2000mm
Uses: metallurgy, electronics, medical, chemical, petroleum, medicine, aerospace, etc.