AWS A5.16 ERTi2 ERTi7 ERTi12 Titanium Welding Filler Rod

AWS A5.16 ERTi2 ERTi7 ERTi12 Titanium Welding Filler Rod

Titanium filler Rod
Titanium welding rod
Titanium Grade 2 Welding Rod
Titanium Welding Filler Wire
ERTi-2 Titanium TIG Welding Rod
Titanium Grade 5 Tig Welding Rod Filler
AWS A5.16 Titanium Alloy Filler
Titanium CP1 Welding Filler Rod
TIG Welding Filler Rods
Titanium TIG Welding Rods
ERTi-1 Titanium Filler Wire
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of aws a5.16 erti2 erti7 erti12 titanium welding filler rod in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

1. Titanium welding filler rod is a metal filler welding wire for Tig welding, it has excellent welding process performance, and beautiful weld formation and its weld metal has excellent comprehensive mechanical properties. It is mainly used for the welding of titanium and titanium alloys.

2. Available criteria and grades

ERTi-1, ERTi-2, ERTi-4, ERTi-5, ERTi-7, and ERTi12 are the grades.

Size: 1.6, 2.0, 2.5, 3.2, 4.0, 5.0, 6.0, 8.0.

Surface treatment: pickling surface, bright surface

State: Annealed state (M) Hot working state (R) Cold working state (Y) (annealed, ultrasonic flaw detection)

Standards: AWS.A5.16

3. What is the characteristic of a titanium welding filler rod?

Surface quality: extremely accurate, well-finished, free of oxidation, and without flaws like peeling, inclusions, thorns, or stains. It's acceptable to have minor localized abrasions, stains, pits, and other imperfections as long as they don't go beyond the wire diameter's authorized deviation.

Surface finish: clean, dust-free, better acid-resistant service life.

Physical characteristics: excellent strength and elongation characteristics; no deformation after cold bending. Wires with a diameter of more than 3mm should be free of shrinkage, pores, delamination, cracks, and metallic or non-metallic inclusions.

ERTi-2 Titanium TIG Welding Rod supplier
Titanium filler Rod price

4. Chemical composition according to AWS A5.16

Chemical symbol markAmerican Standard
AWS A5.16/A5.16M: 2013
Ti99.8ERTi-1
Ti99.6ERTi-2
Ti99.5ERTi-3
Ti99.3ERTI-4
TiPd0.2ERTi-11
TiPd0.6ERTi-17
TiRu0.1ERTI-27
TiPd0.2AERTi-7
TiPd0.6AERTi-16
TiRu0.1AERTi-26
TiNi0.7Mo0.3ERTi-12
TiRu0.05Ni0.05ERTI-15A
TiNi0.5ERTi-13
TiNi0.5AERTi-14
TiNi0.45Cr0.15ERTi-33
TiNi0.45Cr0.15AERTi-34
TiCo0.5ERTi-30
TiCo9.5AERTi-31
TiAl4V2ERTi-38
TiAl6Zr4Mo2Sn2-
TiA18V1Mo-
TiA15V1SnMo1ZrlERTi-32
TiAI3V2.5AERTi-9
TiAl3V2.5RuERTi-28
TiAl3V2.5PdERTi-18
TiAl6V4BERTi-5
TiAl6V4AERTi-23
TiAl6V4Ni0.5PdERTi-25

5. What are titanium welding wire applications?

ERTi-2 Titanium TIG Welding Rod is mainly used in Vacuum salt production, fine chemicals, petrochemicals, pharmaceuticals, Chlor-alkali industry, electroplating, electrolysis, aerospace, desalination, sports equipment, automotive applications, medical implants, hand instruments, construction applications, cladding and other materials, Optical mounts, bolts, and nuts, etc.

   

6. Package and delivery

All customers buy titanium welding filler rods from us, which can be packaged and delivered as the below picture shows, any requests for metal print marking like ERTi2, ERTi7, or ERTi12 are all available.

Packing: Bubble film plus carton or wooden box

Delivery: FedEx, DHL, TNT express delivery door to door or by sea and air freight to your destination.

AWS A5.16 Titanium Alloy Filler price

Hot Tags: aws a5.16 erti2 erti7 erti12 titanium welding filler rod, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Black Surface Titanium Gr1 Wire In Spool For Wire Mesh Making, ERTi 2 Erti 7 Erti 12 Titanium Mig Wire, AWSA5 16 ERTi17 Grade17 Titanium Welding Wires, ERTi 1 ER Ti 2 ER Ti 5 ER Ti 7 ER Ti 9 ER Ti 12 Titanium Filler Wire ASTMB863, Titanium Wire For Anodizing

Send Inquiry

(0/10)

clearall