Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of ansi b16.9 nickel 200/201 nickel pipe fittings in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

Products Introduction

1. Nickel fittings are the general name of nickel elbow, nickel tee, and nickel stub end. It is a pipe fitting made of a kind of corrosion-resistant metal nickel. It plays the role of connection, control, direction change, diversion, sealing, and support in the pipeline system.

2. Basic information

Grade: Ni200 Ni201

Size: 1/2"~24"

Standards: ANSI B16.9

Nickel fittings series products include nickel tee, nickel reducer, nickel elbow, nickel clamp, nickel union, nickel cross, nickel gasket, nickel flange, nickel plug, etc.

Detail Shows

nickel 200 pipe fittings
nickel pipe and fittings

3. Nickel pipe fittings have excellent corrosion resistance to alkaline and neutral solution media of salts such as carbonate, nitrate, oxide, and acetate. It is widely used in the alkali industry, Chlor alkali chemical industry and production of organic chloride, the food processing industry, high-temperature halogen and salt corrosion environment, electronic instrument parts, water treatment, various strong alkali-resistant equipment, etc.

4. Chemical composition of nickel base and iron-nickel base corrosion-resistant alloys

Alloy Ni C Mn Fe S S Cu Cr AI TI Nb Mo others
Ni200 99.5 0.08 0.2 0.2 0.005 0.2 0.1 - - - - -  
Ni201 99.5 0.01 0.2 0.2 0.005 0.2 0.1 - - - - - -
Ni205 99.5 0.08 0.2 0.1 0.004 0.08 0.08 - - 0.03 - - Mg0.05
Ni211 95.0 0.1 4.8 0.4 0.008 0.08 0.1 - - - - -  
Ni220 95.5 0.04 0.1 0.05 0.004 0.03 0.05   - 0.03     Mg0.05
Ni230 95.5 0.05 0.08 0.05 0.004 0.02 0.05     0.003     Mg0.06
Ni270 99.98 0.01 <0.001 0.003 <0.001 <0.001 <0.001 <0.001   <0.001   Co<0.001 Mg<0.001

5. As a professional supplier of nickel pipe and fittings, we not only offer nickel 200 pipe fittings, but also some nickel alloy fittings, such as c276, monel 400, etc, bulk common use nickel fittings stock as below:

Nickel elbow

  • Grade: N4, N6 (Ni200, Ni201)

  • Nickel 200 elbows specification: Φ 19, Φ 25, Φ 32, Φ 38, Φ 45, Φ 50, Φ 57, Φ 76, Φ 89, Φ 108, Φ 133, Φ219

Diameter: 10-1000, thickness: 2.0-10mm.

  • Stock nickel elbow degree: 45°,90°,180°

Nickel tee

  • Grade: N4, N6 (Ni200, Ni201)

  • Nickel 200 elbows specification: Φ 57, Φ 76, etc

  • Support customized production and processing with drawings and samples.

Hot Tags: ansi b16.9 nickel 200/201 nickel pipe fittings, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, brushed nickel tube, copper nickel pipe, nickel 200 pipe, nickel alloy pipe, nickel Butt Weld Fittings, nickel fittings

Send Inquiry

(0/10)

clearall