Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of ni200 ni201 90degree nickel elbow in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Introduction
1. A type of nickel pipe fitting called a nickel elbow has high corrosion resistance because, when exposed to air at normal temperature, the surface oxidizes to form a thick, solid protective film.
2. Basic Information
Nickel pipe elbows size: DN15-DN1200
Bending Radius R=1D, 1.5D, or Custom Pipe Fittings
| Nickel Pipe Fittings Chemical Composition | |||||||
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
| Nickel 200 | 0.15 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
| Nickel 201 | 0.02 max | 0.35 max | 0.35 max | 0.01 max | 0.25 max | 0.40 max | 99.0 min |
3. Pure nickel has excellent welding and processing properties and can be processed into products such as tube rods, wire plates, strips of foil, pipe fittings, and so on. Nickel elbow has good corrosion resistance in NaOH solution of any concentration and temperature and molten NaOH above 400 ℃, it has good room corrosion resistance to Na2O2, Na2CO3, NaHCO3, and alkaline solution or molten liquid containing KNO3.
Detail Shows

nickel pipe elbow

Nickel 200 elbow
4. Applications for nickel elbows include coating various targets for electrodes and constructing chemical equipment such as pipelines, heat exchangers, evaporators, heaters, reactors, etc. Due to its high-temperature toughness, corrosion resistance, thermal expansion qualities, and magnetism, it is particularly employed. ANSI B 16.9 Nickel 201 Pipe Tees have high electrical conductivity and high-temperature resistance.

nickel 200 elbows

Nickel fittings
ASTM B366 Nickel Alloy UNS N02200 Buttweld Reducer is made from commercially pure wrought nickel. Nickel DIN 2.4068 butt welding elbow has good mechanical properties and excellent resistance to many corrosive environments.
Chemical processing and storage typically employ ASME SB 366 Nickel 200 seamless butt welding fittings because of their high quality, great performance, and lack of flaws.