Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of molybdenum wire in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Introduction
1. Molybdenum wire, often known as Moly Wire, is a refractory metal that melts at 4760°F.
2. Basic information
The forming process of molybdenum wires surface state: drawing, forging, and polishing
Features of moly Wire
① Molybdenum wire has high precision, and the wire diameter tolerance is controlled within 0 ~ - 0.002mm;
② Low wire breakage rate, high processing speed, and high-cost performance;
③ It can realize stable long-time continuous processing.
Molybdenum wire employs modern hot and cold drawing combination technology to form high-quality, high-temperature molybdenum raw materials into a linear shape and then uses them as electrodes on wire-cutting machines to process the workpiece.
Detail Shows

Molybdenum wire

3. Chemical composition of molybdenum wire
| Grade | Mo purity% | other elements≤% | Each element≤% | Element content append% |
| Mo1 | 99.95 | 0.05 | 0.01 | / |
| Mo2 | 99.9 | 0.1 | 0.01 | / |
| Mo3 | 99.33 | 0.07 | 0.01 | 0.2-0.6 |
| Grade | description | applications | ||
| MO1 | pure moly wire | It is used in the manufacture of electronic vacuum devices, thermal components, heating elements, different types of bulb hooks, mandrel crimped tungsten wires, etc | ||
| For wire cutting | ||||
| MO2 | pure moly rod | Used in the manufacture of electronic vacuum devices, electrode gas discharge tubes, lamps, and electronic tube supports. | ||
| MO3 | molybdenum with other elements | High-temperature structural materials (printer needle, nut, screw), halogen lamp support, heating wire, and the radial axis of the tube. | ||
4. Moly wires applications:
1. Hot Zones for high-temperature furnaces.
2. Sputtering targets for coating solar cells & flat screens.
3. Glass melting electrodes
4. Heat shields
5. Semiconductor base plates.
6. Brazing fixtures & Boring bars
7. Pigments and catalysts.
5. The manufacturing process of molybdenum wire
Molybdenum wire mainly refers to a consumable made of precious metals such as molybdenum, which is continuously moved with a high-voltage electric field to cut the workpiece during wire cutting. Molybdenum wire has been widely employed as an important metal material in aircraft, the metallurgical chemical industry, mechanical electronics, vehicle manufacture, and other sectors. The production process of molybdenum wire is as follows:
Molybdenum wire is made of metal molybdenum powder as raw material. After obtaining square or round bar-shaped metal molybdenum by powder metallurgy, it is made by rolling, rotary forging, stretching, and other pressure processing and supplemented by various technological means. Finished wire of different varieties and specifications (generally d6.5~0.02mm, and mainly d3.5~0.05mm).

Hot Tags: molybdenum wire, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, molybdenum wire price