Ni201 is a low-carbon nickel plate with lower carbon content, softer, and higher purity than Ni200 nickel plate.
1250x3000x1.0mm nickel plate, bright surface, made of high-purity electrolytic nickel. The thinner the nickel plate and the wider the plate pair, the higher the price. Since nickel itself is not very hard, the processing state includes hard state, semi-hard state, annealed state, etc. The semi-hard state is generally used, which is neither too soft nor too hard, and is easy to transport and process.
In addition to the ni201 nickel plate, we also produce the Ni200 nickel plate, nickel wire, nickel foil, nickel rod, etc. Nickel foil and nickel wire are commonly available in stock. Ni200 is also a pure nickel plate with a higher carbon content than Ni201, a lower purity, and a cheaper price.
The price of nickel plate fluctuates with the nickel price every day. Please contact our sales engineer for details, or send us an inquiry by email.