Home > News > Content

90 Degree Titanium Elbow DN40x3 Shipped To Indonesia

May 10, 2024

On May 9, 2024, the 90-degree 1.5D pure titanium elbow produced by Baoji Fairy Titanium Industry was sent to Indonesia. The Grade 2 titanium elbow produced this time is a commonly used specification in pipeline fittings. In addition, we have also produced titanium flanges, titanium reducers, titanium tees, etc.

90-degree 15D pure titanium elbow

A pushed titanium elbow is made of a seamless titanium tube as the blank, which is pushed and extruded on the push extrusion machine with a tube diameter smaller than the diameter of the finished product. The Northwest Nonferrous Metals Research Institute took the lead in successfully implementing this new technology in the early 1990s. The development of push seamless titanium elbow. We have successfully developed seamless titanium pipe fittings such as titanium tees and reducers. The maximum diameter of seamless pipe fittings can reach Φ114 and meet the requirements of ASTMB363-95 standards.

seamless titanium pipe fittings 90degree elbows

The main application standards for titanium elbows and pipe fittings are ASTMB363, ANSI B16.9, and MSS SP-43. The titanium pipe fittings standard first appeared in the American aerospace standards. The commonly used international standards for titanium pipe fittings in the chemical industry are ASTMB363, and ANSI. B16.9.

ASTMB363 gr2 titanium elbow

In addition to 1.5D, 90-degree titanium elbows also have 1.0D, also known as short-radius titanium elbows. In addition, we can also produce 45-degree and 60-degree titanium elbows, etc. For more about titanium elbows, titanium tees, and titanium pipe fittings, please contact our sales engineer.

Contact information:

Tel: +86-0917- 3664600

Whatsapp: +8618791798690

Email: sales@tmsalloy.com
tina@tmsalloy.com

Send Inquiry