On April 27, 2024, Baoji FairyTitanium Industry shipped 50kg of 0.03x100mm nickel foil to India and South Korea.
0.03mm ultra-thin nickel foil is a high-purity nickel foil prepared by the electrodeposition method. The metal electrodeposition process occurs at the interface between the electrode and the solution. During electrodeposition, the reactants in the solution are transported from the bulk solution to the interface. After surface transformation, electron exchange is carried out at the interface through electrochemical steps to generate a metal coating.
The advantages and applications of electrodeposited nickel foil
Electrodeposited nickel foil has the advantages of a simple process and low cost, with a maximum width of 1300mm, high purity, flexibility, and plasticity. This type of nickel foil is commonly used in electronic devices, conductive materials, heat exchangers, batteries, and other fields. Its main function is to provide conductivity, thermal conductivity, and thermal insulation performance.

Pure nickel foil also has good corrosion resistance, so it can also be used in fields such as chemical engineering and aerospace. Its fine thickness can meet the needs of some special applications.
Contact information:
Tel: +86-0917- 3664600
Whatsapp: +8618791798690