Gr12 ERTi2 Titanium Wire Sent To Italy And The Netherlands

Apr 26, 2024

2024.4.26 Baoji Fairy Titanium Industry Co., Ltd. sent ERTi12 titanium wire 2.5mm to Italy and the Netherlands.

gr12 titanium wire
How to choose titanium welding wire?
When selecting titanium alloy welding wire, you need to consider comprehensive considerations such as the material of the material to be welded, usage requirements, welding process, and other factors. Generally speaking, the selection of welding wire should follow the following principles:
1. The composition is similar to that of the material to be welded. This ensures welding quality and joint performance.
2. Select welding wires of different compositions and diameters according to different process requirements. For example, for welding thick-walled parts, a welding wire with a larger diameter should be selected.

gr12 titanium welding rod
3. Consider the impurity content and surface quality of the welding wire. Impurity content and poor surface quality will affect welding quality and joint performance.
4. Choose welding wires of different hardnesses according to actual needs. Too high a hardness will reduce weldability, and too low a hardness will reduce wear resistance.

gr12 titanium filler wire
Titanium alloy welding wire has good corrosion resistance in most media, is not easy to rust, can withstand large loads, and can easily perform cutting, turning, and other processing operations. It is widely used in aerospace, automobile, chemical industry, and other fields.