| international standard | American standard | Japanese standard | German standard | ||
| alloy symbol | AWS A5.16/A5.16M: 2013 | Aerospace Material Classification | JIS Z3331:2011 | DIN 1737-1: 1984 | |
| digital marker | chemical symbol mark | ||||
| Ti 0100 | Ti99.8 | ERTi-1 | - | STi 0100 | 3.702 6 |
| Ti 0120 | Ti99.6 | ERTi-2 | - | STi 0120 | - |
| Ti 0125 | Ti99.5 | ERTi-3 | AMS 4951:2003 | STi 0125 | - |
| Ti 0130 | Ti99.3 | ERTI-4 | - | STi 0130 | 3.703 6 |
| Ti 2251 | TiPd0.2 | ERTi-11 | - | STi 2251 | 3,7226 |
| Ti 2253 | TiPd0.6 | ERTi-17 | - | STi 2253 | - |
| Ti 2255 | TiRu0.1 | ERTI-27 | - | STi 2255 | - |
| Ti 2401 | TiPd0.2A | ERTi-7 | - | STi 2401 | 3,723 6 |
| Ti 2403 | TiPd0.6A | ERTi-16 | - | STi 2403 | - |
| Ti 2405 | TiRu0.1A | ERTi-26 | - | STi 2405 | - |
| Ti 3401 | TiNi0.7Mo0.3 | ERTi-12 | - | STi 3401 | - |
| Ti 3416 | TiRu0.05Ni0.05 | ERTI-15A | - | STi 3416 | - |
| Ti 3423 | TiNi0.5 | ERTi-13 | - | STi 3423 | - |
| Ti 3424 | TiNi0.5A | ERTi-14 | - | STi 3424 | - |
| Ti 3443 | TiNi0.45Cr0.15 | ERTi-33 | - | STi 3443 | - |
| Ti 3444 | TiNi0.45Cr0.15A | ERTi-34 | - | STi 3444 | - |
| Ti 3531 | TiCo0.5 | ERTi-30 | - | STi 3531 | - |
| Ti 3533 | TiCo9.5A | ERTi-31 | - | STi 3533 | - |
| Ti 4251 | TiAl4V2 | ERTi-38 | - | - | - |
| Ti 4621 | TiAl6Zr4Mo2Sn2 | - | AMS 4952:2007 | STi 4621 | - |
| Ti 4810 | TiA18V1Mo | - | AMS 4955:2008 | STi 4810 | -- |
| Ti 5112 | TiA15V1SnMo1Zrl | ERTi-32 | - | STi 5112 | - |
| Ti 6321 | TiAI3V2.5A | ERTi-9 | - | STi 6321 | - |
| Ti 6324 | TiAl3V2.5Ru | ERTi-28 | - | STi 6324 | - |
| Ti 6326 | TiAl3V2.5Pd | ERTi-18 | - | STi 6326 | - |
| Ti 6402 | TiAl6V4B | ERTi-5 | AMS 4954:2003 | STi 6402 | - |
| Ti 6408 | TiAl6V4A | ERTi-23 | AMS 4956:2003 | ST:6408 | - |
| Ti 6413 | TiAl6V4Ni0.5Pd | ERTi-25 | - | STi 6413 | - |
Titanium welding wires standards AWS A5.16 vs JIS DIN
Apr 09, 2022
Send Inquiry
Categories
Contact Us
Tel: +86-917-3664600
Fax: +86-917-3664600
Email: tina@tmsalloy.com
Add: No.11 South of Baoti Road, Baoji City, Shaanxi Province, P.R. China.