Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of din934 hextitanium nuts in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Introduction
1. Titanium nuts are components that are fastened together using bolts or screws. It is separated into several different categories, including titanium, carbon steel, and stainless steel, depending on the varied materials.
2. Basic Information
Grades 2 and 5 are the most commonly used grades for titanium screws:
• Grade 2 (UNS R50400 / 3.7035): Commercially pure titanium and the most common screw grade.
• Level 5 (UNS R56400 / 3.7165): Excellent strength-to-weight ratio, achieving a unique combination of corrosion resistance and high strength.
Standards: DIN934, ISO, BS, JIS
Type: titanium flange nuts, titanium full nuts, titanium nylon nuts, titanium Hex Nuts, titanium lock nuts, titanium flanged metal locknuts.
3. Titanium fasteners are known for their sturdiness, lightness, and corrosion resistance. They are essential to many industries, including Chlor-alkali, marine, offshore oil and gas, desalination, medical, and pulp and paper.
Detail Shows

Titanium Nuts

Titanium Flanged Nut
4. Titanium nuts size according to DIN934
| Thread Size d | M1 | M1.2 | M1.4 | M1.6 | (M1.7) | M2 | (M2.3) | M2.5 | (M2.6) | M3 | (M3.5) | M4 | M5 | M6 | (M7) | M8 | ||
| P | Pitch | Coarse thread | 0.25 | 0.25 | 0.3 | 0.35 | 0.35 | 0.4 | 0.45 | 0.45 | 0.45 | 0.5 | 0.6 | 0.7 | 0.8 | 1 | 1 | 1.25 |
| Fine thread | / | / | / | / | / | / | / | / | / | / | / | / | / | / | / | 1 | ||
| Fine thread | / | / | / | / | / | / | / | / | / | / | / | / | / | / | / | / | ||
| m | max=nominal size min | 0.8 | 1 | 1.2 | 1.3 | 1.4 | 1.6 | 1.8 | 2 | 2 | 2.4 | 2.8 | 3.2 | 4 | 5 | 5.5 | 6.5 | |
| 0.55 | 0.75 | 0.95 | 1.05 | 1.15 | 1.35 | 1.55 | 1.75 | 1.75 | 2.15 | 2.55 | 2.9 | 3.7 | 4.7 | 5.2 | 6.14 | |||
| MW | min | 0.44 | 0.6 | 0.76 | 0.84 | 0.92 | 1.08 | 1.24 | 1.4 | 1.4 | 1.72 | 2.04 | 2.32 | 2.96 | 3.76 | 4.16 | 4.91 | |
| s | max=nominal size min | 2.5 | 3 | 3 | 3.2 | 3.5 | 4 | 4.5 | 5 | 5 | 5.5 | 6 | 7 | 8 | 10 | 11 | 13 | |
| 2.4 | 2.9 | 2.9 | 3.02 | 3.38 | 3.82 | 4.32 | 4.82 | 4.82 | 5.32 | 5.82 | 6.78 | 7.78 | 9.78 | 10.73 | 12.73 | |||
| e ① | min * | 2.71 | 3.28 | 3.28 | 3.41 | 3.82 | 4.32 | 4.88 | 5.45 | 5.45 | 6.01 | 6.58 | 7.66 | 8.79 | 11.05 | 12.12 | 14.38 | |
| - | - | - | - | - | - | - | - | - | - | - | - | - | - | - | - | |||
| per 1000 units ≈ kg | 0.03 | 0.054 | 0.063 | 0.076 | 0.1 | 0.142 | 0.2 | 0.28 | 0.72 | 0.384 | 0.514 | 0.81 | 1.23 | 2.5 | 3.12 | 5.2 | ||
| Thread Size d | M10 | M12 | (M14) | M16 | (M18) | M20 | (M22) | M24 | (M27) | M30 | (M33) | M36 | (M39) | M42 | (M45) | M48 | ||
| P | Pitch | Coarse thread | 1.5 | 1.75 | 2 | 2 | 2.5 | 2.5 | 2.5 | 3 | 3 | 3.5 | 3.5 | 4 | 4 | 4.5 | 4.5 | 5 |
| Fine thread | 1 | 1.5 | 1.5 | 1.5 | 1.5 | 2 | 1.5 | 2 | 2 | 2 | 2 | 3 | 3 | 3 | 3 | 3 | ||
| Fine thread | 1.25 | 1.25 | / | / | 2 | 1.5 | 2 | / | / | / | / | / | / | / | / | / | ||
| m | max=nominal size min | 8 | 10 | 11 | 13 | 15 | 16 | 18 | 19 | 22 | 24 | 26 | 29 | 31 | 34 | 36 | 38 | |
| 7.64 | 9.64 | 10.3 | 12.3 | 14.3 | 14.9 | 16.9 | 17.7 | 20.7 | 22.7 | 24.7 | 27.4 | 29.4 | 32.4 | 34.4 | 36.4 | |||
| MW | min | 6.11 | 7.71 | 8.24 | 9.84 | 11.44 | 11.92 | 13.52 | 14.16 | 16.56 | 18.16 | 19.76 | 21.92 | 23.52 | 25.9 | 27.5 | 29.1 | |
| s | max=nominal size min | 17 | 19 | 22 | 24 | 27 | 30 | 32 | 36 | 41 | 46 | 50 | 55 | 60 | 65 | 70 | 75 | |
| 16.73 | 18.67 | 21.67 | 23.67 | 26.16 | 29.16 | 31 | 35 | 40 | 45 | 49 | 53.8 | 58.8 | 63.1 | 68.1 | 73.1 | |||
| e ① | min * | 18.9 | 21.1 | 24.49 | 26.75 | 29.56 | 32.95 | 35.03 | 39.55 | 45.2 | 50.85 | 55.37 | 60.79 | 66.44 | 71.3 | 76.95 | 82.6 | |
| - | - | - | - | - | - | - | - | - | - | - | - | - | - | - | - | |||
| per 1000 units ≈ kg | 11.6 | 17.3 | 25 | 33.3 | 49.4 | 64.4 | 79 | 110 | 165 | 223 | 288 | 393 | 502 | 652 | 800 | 977 | ||
| Thread Size d | (M52) | M56 | (M60) | M64 | (M68) | M72 | (M76) | M80 | (M85) | M90 | M100 | M110 | M125 | M140 | M160 | |||
| P | Pitch | Coarse thread | 5 | 5.5 | 5.5 | 6 | 6 | / | / | / | / | / | / | / | / | / | / | |
| Fine thread | 3 | 4 | 4 | 4 | / | 6 | 6 | 6 | 6 | 6 | 6 | 6 | 6 | 6 | 6 | |||
| Fine thread | / | / | / | / | 4 | 4 | 4 | 4 | 4 | 4 | 4 | 4 | 4 | / | / | |||
| m | max=nominal size min | 42 | 45 | 48 | 51 | 54 | 58 | 61 | 64 | 68 | 72 | 80 | 88 | 100 | 112 | 128 | ||
| 40.4 | 43.4 | 46.4 | 49.1 | 52.1 | 56.1 | 59.1 | 62.1 | 66.1 | 70.1 | 78.1 | 85.8 | 97.8 | 109.8 | 125.5 | ||||
| MW | min | 32.3 | 34.7 | 37.1 | 39.3 | 41.7 | 44.9 | 47.3 | 49.7 | 52.9 | 56.1 | 62.5 | 68.6 | 78.2 | 87.8 | 100 | ||
| s | max=nominal size min | 80 | 85 | 90 | 95 | 100 | 105 | 110 | 115 | 120 | 130 | 145 | 155 | 180 | 200 | 230 | ||
| 78.1 | 82.8 | 87.8 | 92.8 | 97.8 | 102.8 | 107.8 | 112.8 | 117.8 | 127.5 | 142.5 | 152.5 | 177.5 | 195.4 | 225.4 | ||||
| e ① | min * | 88.25 | 93.56 | 99.21 | 104.86 | 110.51 | 116.16 | 121.81 | 127.46 | 133.11 | 144.08 | 161.02 | 172.32 | 200.57 | 220.8 | 254.7 | ||
| - | - | - | - | - | - | - | - | - | - | - | 170 | 196 | 216 | 248 | ||||
| per 1000 units ≈ kg | 1220 | 1420 | 1690 | 1980 | 2300 | 2670 | 3040 | 3440 | 3930 | 4930 | 6820 | 8200 | 13000 | 17500 | 26500 | |||

Hot Tags: din934 hextitanium nuts, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Grade2 Titanium Hex Allen Socket Button Head Screws, Gr2 Gr5 Titanium Socket Head Cap Screws DIN 912, DIN 7976 Gr5 Titanium Self Tapping Screws, Gr2 M8x30mm Pure Titanium Fully Threaded Studs Rods DIN 975, DIN 912 Grade2 Titanium Allen Button Head Bolts