Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of astm f136/f67 medical titanium bar in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Introduction
1. Medical titanium bar is a metal solid bar used for medical implants or medical devices, such as artificial joints, bone plates, screws, and surgical instruments.
2. What is the grade of the medical titanium bar?
Pure titanium: Gr1 Gr4
Titanium alloy: Gr23 Gr5ELI (TA6V ELI)
3. Standards of titanium bar for medical use:
ASTM F136 for titanium alloy
ASTMF67 for pure titanium
4. Chemical elements and Mechanical Properties according to ASTMF136
| Element | Composition,% |
| Nitrogen, max | 0.05 |
| Carbon, max | 0.08 |
| Hydrogen, max | 0.012 |
| Iron, max | 0.25 |
| Oxygen, max | 0.13 |
| Aluminum | 5.5-6.50 |
| Vanadium | 3.5-4.5 |
| Titanium | balance |
| Nominal Diameter or Distance | Tensile Strength min, | Yield Strength m | Elongation | Reduction |
| Between Parallel Sides, in. (mm) | psi(MPa) | (0.2% offset Min,psi(MPa) | L | L |
| Under 0.187 (4.75) thickness or diameter | 860 | 795 | 10 | --- |
| 0.187(4.75) to under 1.75(44.45),incl | 860 | 795 | 10 | 25 |
| 1.75 (44.45) to under 2.50(63.50),incl | 825 | 760 | 8 | 20 |
| 2.50(63.50) to 4.00(101.60),incl | 825 | 760 | 8 | 15 |

5. What are the advantages of medical titanium bar?
Medical titanium rods have low density, are lightweight, have high strength, have good biocompatibility with the human body, and the material is corrosion-resistant in the human environment.
6. Our advantages
We have complete processing equipment and rich processing experience. The medical titanium rods all have been tested by a third party (chemical composition, mechanical properties, metallographic structure, tolerance), polished and polished rods have undergone flaw detection treatment and the product quality stabilize. it is mainly used in machinery equipment, electroplating equipment, medical, various precision parts, and other industries.

7. Other related titanium bars for medical applications
Medical titanium bars are widely used in the medical industry due to their high biocompatibility and corrosion resistance. These bars are made from pure titanium or titanium alloys such as Ti-6Al-4V, Ti-6Al-7Nb, and Ti-13Nb-13Zr, among others. The following are some product descriptions of medical titanium bars:
Pure Titanium Bar: It is a medical-grade titanium bar that is 99.5% pure. Pure titanium bars are used in surgical implants, dental implants, and other medical devices.
Ti-6Al-4V Bar: This is the most commonly used titanium alloy for medical implants because it is lightweight, strong, and biocompatible. It is used in the manufacture of orthopedic implants, bone screws, dental implants, and spinal fixation devices.
Ti-6Al-7Nb Bar: This alloy has excellent biocompatibility, making it ideal for medical implants such as artificial knee and hip joints. Its high strength and corrosion resistance also make it a popular choice for dental implants.
Ti-13Nb-13Zr Bar: This alloy is often used in the manufacture of orthopedic implants and dental implants. It has a low modulus of elasticity, which reduces stress on the surrounding bone tissue.
Medical titanium bars are essential components in the manufacturing of medical devices and implants. They offer exceptional biocompatibility, corrosion resistance, and strength, making them ideal for use in the human body.
Hot Tags: astm f136/f67 medical titanium bar, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Precision Titanium Round Bar Rod Ti 6Al 4V ELI, Titanium Grade 5 (6AL4V) bar, ASTMF136 Gr5ELI Gr23 Medical Titanium Rods, Timascus Rod Damascus Titanium Rod, 10mm TA6V Grade 5 Titanium Rod, Titanium Rectangular Bar Or Rec Bar