Niobium Tubes And Niobium Discs Were Shipped To India

Sep 11, 2024

On September 10, 2024, niobium tubes and niobium disks were shipped to India by Baoji Fairy Titanium Industry Co., Ltd. Niobium tubes are a rare high-melting-point metal that is silver-gray, soft, and ductile. At room temperature, niobium does not react with air, and will not be completely oxidized when it is red-hot in oxygen.

Niobium can directly combine with sulfur, nitrogen, and carbon at high temperatures. Niobium does not react with inorganic acids or alkalis nor dissolve in aqua regia, but it is soluble in hydrofluoric acid. Because niobium has good superconductivity, high melting point, corrosion resistance, wear resistance, and other characteristics, it is widely used in steel, superconducting materials, aerospace, atomic energy, and other fields.

Niobium tubes niobium disc supplier

Niobium tube and niobium disc purity: 99.95%-99.99%
Grade: R04200, R04210, Nb1, Nb-Ti
Standard: ASTM B393-05 ASTM B394-98
32x2, 52x2 niobium tube is a commonly used seamless pure niobium tube, which can be used to make niobium protection tubes, vacuum blast furnace heating components, insulation components charging vessels, etc.

Niobium disc is cut and processed from pure Niobium bars. Due to its excellent high-temperature resistance and good electrical and thermal conductivity, it can be used to manufacture high-temperature furnaces, high-temperature containers, electronic devices radiators, etc.

For more information about the price of niobium rods, niobium tubes, and niobium discs, please contact our sales engineer.