High Purity ED Nickel Foil delivery to the customer
The high purity nickel foil is finished and delivered to the customer on 29 August 2022, pure nickel foil produced by electrodeposition has good compactness, surface finish, and high purity, and its magnetic and mechanical properties are better than those of traditional rolled thin strip.

Electrodeposited Nickel Foil
Thickness: 0.005mm/5um
Thickness range: 5~50um
Purity: Ni >99.96%
Density:8.91g/cm3
Thickness tolerance:0~+0.0015mm
Max width: 1200mm
Status: in coil
Surface and color: nickel silver bright surface