There are many types of titanium pipe fittings, so various processing methods will be used. What are the specific processing methods? Now listen to the introduction of titanium pipe fitting manufacturers.
Forging method: stretch the end or part of the pipe with a swaging machine to reduce the outer diameter. The commonly used swaging machines are rotary, connecting rod and roller.
Stamping method: expand the pipe end to the required size and shape with a tapered core on the punch.
Roller method: place the core in the pipe, and push the periphery with a roller for processing round edges.
Rolling method: generally, the mandrel is not used, and it is suitable for the inner circular edge of a thick wall pipe.

Bending forming method: there are three commonly used methods, one is called the stretching method, the other is called stamping method, and the third is the familiar roller method. There are 3-4 rollers, two fixed rollers, and one adjustment roller to adjust the fixed roller distance. The finished pipe fittings are bent. This method is widely used. If spiral tubes are produced, the curvature can also be increased.
Bulging method: one is to place rubber in the tube and compress it with a punch to make the tube bulge into shape; The other method is hydraulic bulge forming. Fill the middle of the pipe with liquid, and the liquid pressure will bulge the pipe into the desired shape. (The content is for reference only. If you have problems or encounter problems, please consult online or call us. We will serve you wholeheartedly.)