Molybdenum wire is a wire-cut material that uses an advanced hot-cold drawing process to process high-quality high-temperature molybdenum raw materials into filaments. There are many kinds of molybdenum wire, which can be mainly divided into pure molybdenum wire, lanthanum molybdenum wire, yttrium molybdenum wire, and wire cutting professional molybdenum wire.

1) Pure molybdenum wire

The purity of molybdenum in pure molybdenum wire is as high as 99.95% or more, which is usually used for heating components, brackets, auto parts spraying, molybdenum foil strips and wire winding-core wires, etc.;

2) Lanthanum molybdenum wire

Lanthanum molybdenum wire is a molybdenum wire doped with lanthanum. It is mainly used for molybdenum foil strips, furnace heating materials, wire-wound core wire glass seals, and as a wire-cutting high-temperature component.

3) Yttrium molybdenum wire

Yttrium molybdenum wire is mainly used in electronic tube reeds, furnace heating materials, grids, brackets, lead wires, etc.;

4) Molybdenum wire for wire cutting

Molybdenum wire for wire cutting is a kind of molybdenum wire with a high surface finish, high strength, long service life, good discharge performance, and fast cutting speed. It is principally used for cutting various non-ferrous metals,  steeland magnetic materials. 