| ASTM B265 | Strip, Sheet, and Plate |
| ASTM B338 | Seamless Welded Tubes |
| ASTM B348 | Bar and Billet |
| ASTM B363 | Fittings |
| ASTM B367 | Castings |
| ASTM B381 | Forgings |
| ASTM B861 | Seamless Pipe |
| ASTM B862 | Welded Pipe |
| ASTM F67 | Unalloyed Titanium for Surgical Implants |
| AWS A5.16 | Weld Wire |
| ISO 5832-2 | Unalloyed Titanium for Surgical Implants |
Titanium and titanium alloy US standards of different products