Common process flow and contents of Ti-6AL-4V Grade 5 Titanium plate cutting are described as follows:
Titanium plate
(1) If semi-automatic cutting is carried out, then the guide rail should be placed on the flat surface of the titanium plate, the cutting machine should be placed on the guide rail, paying attention to the sequence can not be reversed.
(2) The cutting parameters of the Ti-6AL-4V Grade 5 Titanium plate should be properly determined according to the thickness of the plate, etc. in order to obtain a good cutting effect.
(3) Check whether the cutting tip is smooth or not. If there is any blockage, it should be cleared in time.
(4) The plate should be cleaned before cutting, and there should be a certain space left, which can facilitate the blowing out of slag.
(5) The distance between the cutting nozzle and the surface of the plate should be suitable, too close or too far is not good.
(6) Preheat the plate sufficiently to avoid affecting the cutting process.
(7) If different sizes of work are cut, small pieces should be cut first and then large pieces.