Preparation of chlorine dioxide by electrolysis of titanium anode

Dec 21, 2022

Titanium Anode for Electrolysis of Chlorine Dioxide

Titanium anodes for the electrolysis of chlorine dioxide have the following advantages

1. When chlorine dioxide is produced by titanium anode electrolysis, it also generates 03, CL2, H202, and other strong oxidizing and widespread bactericidal abilities. The disinfection effect is far better than that of the chemical method.

2. Low cost of electrolysis disinfection

3. Good safety, safe transportation, storage, and operation of production raw materials. Chlorine is used for the chemical production of chlorine dioxide. However, the transportation and storage of chlorine are inconvenient. More importantly, there are great potential safety hazards

4. Easy source of raw materials: chlorine dioxide is produced by electrolysis. The principle is to use a drinking anode to electrolyze salt water, which is more convenient and safer than chlorine salt water

For chlorine dioxide generators, ruthenium iridium coating plate titanium anode is generally used, and our company provides customized special-shaped parts.