Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of grade9 titanium bike frame in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
1. Grade9 titanium bike frame is a bike frame which is made of titanium alloy 3al2.5v, it is ultra-light and corrosion-resistant better than stainless steel and aluminum alloy.
2. Size and parameters
Grade: Gr9
Weight: 1.4~1.7kg
Size: 26" 27.5" 29"
Head pipe: 41.8-52 concealed conical head pipe / 44 straight head pipe


3. The chemical and mechanical properties of Grade9 titanium bike frame
| Grade | N | C | H | Fe | Al | V | O | Ti |
| Gr9 | 0.02 | 0.05 | 0.013 | 0.25 | 2.5~3.5 | 2.0~3.0 | 0.12 | balance |
| Grade | tensile strength | yield strength | Elongation (%) |
| Gr9 | 620 | 485 | 15 |
4. What are the advantages of grade9 titanium bike frame?
The fatigue limit of titanium alloy is twice that of steel, and the frame cannot be compared with the titanium alloy frame in this respect after a long period of use. As a high-strength and low-density titanium alloy material used in bicycle frames, it Not only will it make the frame lighter and stronger, but it will also make the frame more durable.
5. Our advantages
Except for titanium mtb frame, titanium road bike frame, titanium bmx frame, titanium small wheel frames, we also provide titanium bicycle brakes, titanium forks, titanium water bottle cages, titanium spokes, bicycle titanium screws, etc. Welcome to buying Grade9 titanium bike frame, inquiry pls send to sales@tmsalloy.com

Hot Tags: grade9 titanium bike frame, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, High Strength Gr2 Grade 5 TA6V ELI Titanium Balls, Grade 5 Extended Titanium Tension Spring Small Dual Hook Titanium Springs, Ruthenium Iridium Coated Titanium Felt, PEM Electrolysis Platinized Titanium Fiber Felt