What is a glass-melting electrode?
The glass-melting molybdenum electrode is used in the glass furnace for producing high-quality glass and glass fiber.
Glass melting electrode material
The glass melting electrode must be able to withstand extremely high temperatures and aggressive glass melting. Molybdenum is the most suitable material to meet these challenging conditions, based on the characteristics:
1. Melting point 2620 ° C
2. High purity
3. Excellent creep resistance
4. Dimensional stability
5. Excellent corrosion resistance
6. Good conductivity and thermal conductivity
Application of Molybdenum Electrode to Glass
1. Water cups, food containers, and tableware;
2. Glass windows of homes, offices, and vehicles;
3. Electronic panel of display and solar cell;
4. Various industrial and scientific containers.