Tungsten Bar

Tungsten Bar

Tungsten round bar
Tungsten bar stock
Tungsten bar price
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of tungsten bar in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

Products Introduction

1. Tungsten Bar also named tungsten rod, is made of metal powder at specific high temperatures, using special high-temperature powder metallurgy technology.

2. Basic information

Grade: W1, W2, W3, W4
Tungsten bar DIA: (2.0-100.0mm)
Length: 50-1000mm
Density: 19.28 g/cm³

Purity 99.92%, 99.98% also available

Tungsten round bar Surface: Sintering surface, Forged surface, Ground surface.

Detail Shows

TUNGSTEN bar

Pure Tungsten Bar

Tungsten Rod

99.95% tungsten bars

3. Pure Tungsten Bar has been widely used in various tungsten electrodes, printer needles, support wires, lead-in wires, quartz furnace heating devices, filaments, high-speed steel, welding, etc.

The special properties of tungsten rods include low thermal expansion, good thermal conductivity, sufficient electrical resistance, high elastic modulus, etc.

The tungsten bars with a purity of 99.95% are used primarily to cast raw materials for ingredients and forging special steel and drawn steel wires.

4. Corresponding chemical composition of tungsten rod

GradeW≥%K≥%Other element content
FeAlMoSiAs/Ca/Cr/MgBi/Cd/Cu/Pb
≤%≤%≤%≤%/Mn/Na/Ni/Sb/Co/Ti/Sn
WK8099.950.007-0.0090.0020.0030.0030.0015≤0.001≤0.0005
WK6099.950.005-0.0070.0020.0030.0030.0015≤0.001≤0.0005
WK4099.950.003-0.0050.0030.0030.0030.0015≤0.001≤0.0005
W199.95<0.00150.0030.0030.0030.0015≤0.001≤0.0005

5. Production process of tungsten rod: sintering → forging → rotary forging → rolling → polishing → finished product packaging.

Hot Tags: tungsten bar, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Tungsten Nickel Iron Rod W Ni Fe Alloy

Send Inquiry