Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of sintered porous plate 1mm thickness titanium porous metal sintered plate in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Description Tel:0917-3664600
Titanium porous metal sintered plates are made from titanium powder through the process of cold pressing, sintering, and hot pressing. This manufacturing technique produces a product that is highly porous with a range of pore sizes and interconnected channels to maximize filtration efficiency.
Product features:
Some key features of titanium porous metal sintered plates include:
High porosity: The porosity of titanium porous metal sintered sheets ranges from 30% to 50%, which enables effective filtration while allowing for high flow rates.
Chemical resistance: Titanium is known for its excellent corrosion resistance in a broad range of acidic and alkaline environments, which makes it suitable for use in a wide range of industrial applications.
High temperature resistance: Titanium sintered plates have a high melting point of 1668°C, allowing these plates to perform well in high-temperature applications.
Durability: Titanium sintered sheets are durable and resistant to wear, which makes them suitable for applications where the filtration material may experience high stress or be subjected to frequent cleaning cycles.
Customizability: Titanium porous metal sintered plates can be customized to meet specific filtration requirements, including pore size, thickness, and shape.

Specification Tel:0917-3664600
| Grade | Gr1 pure titanium |
| Size | 0.5mm to 10mm; 1μm to 100μm; |
| Porosity | 20% to 60% |
| Melting point | 1668°C |
Factory Tour Tel:0917-3664600



Common use titanium sintered porous plate Tel:0917-3664600
The grade of titanium used to produce the porous metal sintered plate is typically Grade 1, which is a commercially pure form of titanium that has excellent corrosion resistance and good mechanical properties.
The product parameters of titanium porous metal sintered plate can vary depending on the application. Some common parameters include thickness, pore size, and porosity. The thickness can range from 0.5mm to 10mm, while the pore size can range from 1μm to 100μm. The porosity, or the ratio of the void volume to the total volume, can range from 20% to 60%.
Applications of titanium sintered porous sheet Tel:0917-3664600
The applications of titanium porous metal sintered plate are varied and can include filtration, gas and liquid diffusion, catalyst support, and electrode materials in electrochemical systems. Due to its high surface area, the material is often used in biomedical applications such as bone implants and tissue engineering scaffolds. It is also utilized in the aerospace industry for applications such as heat exchangers and acoustic damping materials. Overall, Sintered titanium metal sheet offers excellent mechanical, thermal, and chemical stability, making it a versatile material for a range of applications.
Packing And Shipping Tel:0917-3664600


Other related sintered titanium metal sheet and porous titanium disc
Hot Tags: sintered porous plate 1mm thickness titanium porous metal sintered plate, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, CT23755 87 Ti 5AL 2 5Sn Gr6 BT5 1 Titanium Plate, ASTMB265 Ti 0 05Pd Gr17 Titanium Plate, ASTMB265 Ti 0 05Pd Gr16 Titanium Sheet, ASTMB265 Ti 0 2Pd Gr11 Titanium Plate, Sintered Porous Plate 1Mm Thickness Titanium Porous Metal Sintered Plate, ASTMB265 3 7105 UNS R53400 Gr12 Titanium Sheet