Ti-3Al-2.5V ASTMB265 Gr9 Titanium Sheet

Ti-3Al-2.5V ASTMB265 Gr9 Titanium Sheet

Grade 9 Titanium Sheet
Titanium Alloy Gr 9 Sheets
Titanium Alloy Ti-3Al-2.5V (Grade 9) plate
UNS R56320 Titanium
ASTM B265
MOQ stock for 1 piece
Send Inquiry
Chat Now
Description

Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of ti-3al-2.5v astmb265 gr9 titanium sheet in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.

 

1. Gr9 titanium sheet is a kind of α alloy with 3% and 2.5% V (Ti 3Al-2.5V), it is also called half Gr5 alloy (Ti6al4v), its tube is mainly used as a titanium bike frame, and the titanium sheet is used in the aerospace field.

2. Size and specifications:

Size: 1000X2000, etc 

Thick: 1.0~60mm 

Standards: ASTMB265 ASTME, AMS4911 

3. Feature of the Gr9 titanium sheet 

Good room and high-temperature mechanical properties and corrosion resistance

Titanium Grade 9 plate also has excellent cold and hot working process plasticity, formability, and weldability. 

It is insensitive to notch and has a good match with the strength and stiffness of composites, which can further achieve a good weight reduction effect.

Gr9 titanium sheet supplier
Gr9 titanium sheet price

4. Chemical and physical properties 

Grade C O N H Fe Al V Residual max each  Residual max total
UNS R56320 GR9 0.08 0.15 0.03 0.015 0.25 2.5~3.5 2.0~3.0 0.1 0.4
Grade Tensile strength Mpa yield strength  0.2%  Mpa Elongation %
GR9 620 483 15

5. Applications 

The strength of Gr9/TA18 titanium alloy is 20%-50% higher than that of pure titanium at room and high temperatures, and its weldability and cold formability are better than those of Gr5/TC4 alloy. The maximum operating temperature is about 315 ℃. Although the strength of this alloy is not as high as that of grade 5 alloy, it is widely used because of its excellent cold-working properties. Gr9 titanium alloy plate, strip, and foil are used in the aircraft honeycomb structure, and can also be used as other parts requiring strength, cold forming, and welding structure.

ASTMB265 Gr9 titanium sheet supplier

6. Our advantages 

We have raw material stock, titanium grade 9 sheet and plate can be ordered by customer's request, 1.0mm thick Titanium Sheet - Grade 9 in stock(1000x2000 or 1100x2200mm), other thick materials like 4mm, 5mm, and 6mm, some sizes in stock, 3rd party material test supported, contact us to get the Grade 9 titanium sheet price at sales@tmsalloy.com

7. FAQ

Q: 1. What are the core advantages of GR9?

A: If GR1 is the gentle, "pure plastic" type, and GR5 (TC4) is the tough, high-strength ace, then GR9 is the well-rounded "all-rounder." Its advantages lie in:
* Excellent processability: It possesses excellent cold formability (cold working performance) and weldability, with its cold formability even surpassing that of the ace alloy GR5 (TC4). This makes it ideal for manufacturing parts requiring complex bending and stamping.
* Strength advantage: Its room temperature strength is 20% to 50% higher than that of industrial pure titanium (such as GR1 and GR2), far exceeding that of pure titanium.
* Excellent corrosion resistance: In seawater, salt spray, and various chemical media, its corrosion resistance is very close to that of pure titanium.
* Superior overall performance: GR9 achieves a good balance between strength, processability, and corrosion resistance.

Q: 2. What is the difference between GR9 and GR2 (TA2)?

A: GR2 (pure titanium): The "all-rounder," with the best overall corrosion resistance and processability, offering the highest cost-effectiveness, and widely used in various civilian fields.
GR9 (Titanium Alloy): With the addition of aluminum and vanadium, its strength is significantly higher than GR2, making it suitable for applications requiring higher strength. While its machinability is better than GR5, it is still slightly inferior to pure titanium.
In short: If you find GR2 insufficiently strong but don't need a material as strong as GR5, GR9 is the ideal middle ground.

Q: 3. How to choose between GR9 and GR5 (TC4)?

A: This is the most common comparison question.
Strength difference: GR5 has significantly higher strength than GR9, with tensile strength exceeding 900 MPa. GR9, while maintaining a certain level of strength, offers better cold formability and weldability.
Machining performance: Due to its high strength, GR5 alloy is difficult to machine and is typically used to manufacture structural components that do not require complex forming. GR9 is ideal for manufacturing pipes or components that require complex cold forming.
In short, Choosing GR5 means pursuing the ultimate in ultra-high strength and high heat resistance; choosing GR9 means needing a perfect balance between strength and good cold workability. GR9 is also more resistant to marine corrosion.

Q: 4. What are GR9 titanium plates used for in marine engineering?

A: GR9 exhibits excellent corrosion resistance in seawater (far superior to stainless steel) and is commonly used in the manufacture of seawater pipelines, heat exchanger tube bundles, and pressure hulls for deep-sea submersibles, significantly improving the economic efficiency throughout the equipment's life cycle.

Q: 5. What are the applications of GR9 titanium plates in the chemical industry?

A: Combining excellent corrosion resistance and good heat transfer properties, it is used in the manufacture of critical equipment such as heat exchangers, reactors, and evaporators, effectively resisting corrosion from various acidic and alkaline media.

Contact Us

Tel: +86-0917- 3664600

Fax: +86-0917- 3664600

WhatsApp: +8618791798690

Mail: sales@tmsalloy.com

tina@tmsalloy.com 

Hot Tags: ti-3al-2.5v astmb265 gr9 titanium sheet, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ASTMB265 Ti 0 05Pd Gr17 Titanium Plate, ASTMB265 3 7105 UNS R53400 Gr12 Titanium Sheet, ASTMB265 Ti 0 05Pd Gr16 Titanium Sheet, Sintered Porous Plate 1Mm Thickness Titanium Porous Metal Sintered Plate, CT23755 87 Ti 5AL 2 5Sn Gr6 BT5 1 Titanium Plate, ASTMB265 Ti 0 2Pd Gr11 Titanium Plate

Send Inquiry

(0/10)

clearall