Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of titanium steel clad tube sheet in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
1. Titanium steel-clad tube sheet is made of explosion-bonded titanium steel-clad plate, which is drilled and machined after the CNC process for heat exchanger applications.
2. Titanium steel clad tube sheet size and diameters
Grade: Q235B+Gr1 SS304+Gr1 etc
Other common base course materials: Q235A (B), Q345A (B), 20R, 16MnR, etc
Other common cladding materials 0cr17, 0Cr18Ni9, 0Cr18N10Ti, 1cr18N9T, 00cr17N14Mo2, etc
Thickness: > 3mm, in which the thickness of the composite layer is 1mm~6mm,
Width: 1500mm~2600mm Length:<12000mm
Bonding rate: not less than 98%
Status: hot rolling, heat treatment, or polishing.
Tube sheet tolerance: as per the customer's drawings
Standards: ASMTB265 NB/T47002.3-2009


3. The manufacturing process and advantages of titanium steel-clad tube sheet
Titanium steel composite plate is a new type of bimetallic high-efficient energy-saving material, which is made of titanium material as the cladding, carbon steel or low alloy steel as the base, and is made of explosive composite method or rolling and crimping method. Titanium steel clad tube sheet has the high strength of ordinary steel plate and the corrosion resistance of coated titanium metal. It can not only save a lot of titanium materials but also have the properties that any single metal does not have. Therefore, compared with pure titanium, the equipment barrel, tube sheet, and head made of titanium composite plate can not only ensure performance but also significantly reduce the project cost. In recent years, titanium composite plate has been widely used in the petrochemical industry, metallurgy, offshore engineering, and other fields, among which the application in salt making and chemical manufacturing is increasing.

4. The application of titanium steel-clad tube sheet
Specific application scope: power plant, pressure vessel, storage tank, reaction tank, desulfurization equipment, anti-corrosion pipeline, water tank, etc.

5. FAQ welcome to inquiry
1. Are you a manufacturing or trading company?
We are a titanium manufacturer, started in 2019.
2. Do you have a dedicated R & D team? Can you design a product for us?
our own professional technical team who has been cooperating closely with a local university on researching and developing tube sheets for several years. We will according to your required drawing make the product for you.
3. What is your payment method?
We can accept T/T, LC, western union, etc, samples accepted.
4. How long is your delivery time?
Inventory samples: within 3 working days
Products for bulk orders: 25-30 workdays

Hot Tags: titanium steel clad tube sheet, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, Stainless steel clad tube-sheet, Titanium Clad Tube Sheet Plates, Titanium-stainless Clad Steel Plates, Ti clad copper bar, Gr.1 Titanium Clad Plate, Gr.1 Titanium Carbon Steel Clad Tubesheet