Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of astmb265 waterjet cutting gr2 gr12 titanium circles in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
Products Description Tel:0917-3664600
Titanium circles made from Gr2 and Gr12 are commonly used in various applications, such as in the aerospace industry, medical equipment, and chemical processing.
Product features: Gr2 titanium circles have excellent corrosion resistance, formability, and weldability, making them ideal for applications that require good ductility and a high strength-to-weight ratio. Gr12 titanium circles have a higher strength-to-weight ratio and can withstand higher temperatures compared to Gr2, making them suitable for applications that require high strength and elevated temperature resistance.

Specification Tel:0917-3664600
| Grade | Gr2 Gr5 Gr12 titanium |
| Size | 500, 600mm, etc |
| Surface | sandblasting or pickling surface |
| Standards | AMS 4911 and ASTM B265 |
Product Pictures Tel:0917-3664600



Chemical composition of Gr2 Gr5 Gr12 titanium Tel:0917-3664600
| Elements(%) | Gr2 | Gr5 | Gr12 |
| N | 0.03 | 0.05 | 0.03 |
| C | 0.08 | 0.08 | 0.08 |
| H | 0.015 | 0.015 | 0.015 |
| Fe | 0.3 | 0.4 | 0.3 |
| O | 0.25 | 0.2 | 0.25 |
| Al | 5.5~6.75 | ||
| V | 3.5~4.5 | ||
| Mo | 0.2~0.4 | ||
| Ni | 0.6~0.9 | ||
| Single | 0.1 | 0.1 | 0.1 |
| Total | 0.4 | 0.4 | 0.4 |
Applications of Titanium Circles
Titanium circles are widely used in various industrial applications due to their excellent properties, such as high strength-to-weight ratio, corrosion resistance, and low thermal expansion coefficient
Aerospace Industry: Titanium circles are extensively used in the aerospace industry for manufacturing aircraft components, such as engine parts, landing gears, and structural elements. The use of titanium circles in the aerospace industry is mainly due to its high strength-to-weight ratio, excellent corrosion resistance, and good fatigue resistance.
Chemical Processing Industry: Titanium circles are used in chemical processing and petrochemical industries to manufacture heat exchangers, pressure vessels, and other equipment that come in contact with corrosive chemicals. Titanium's high corrosion resistance and ability to withstand extreme temperatures and pressures make it an ideal material for these applications.
Marine Industry: Titanium circles are also employed in the marine industry for manufacturing ship hulls, propellers, and other components that require high corrosion resistance and strength-to-weight ratio.
Packing And Shipping Tel:0917-3664600
Package and delivery have become essential aspects of modern-day commerce. With the rise of e-commerce, online shopping has become increasingly popular, and package and delivery services have become a crucial component of the supply chain.
Package and delivery refer to the process of transporting goods from one place to another through various means such as postal services, courier companies, and logistics providers. The primary objective of package and delivery is to ensure that the goods are delivered to their intended recipients in a timely, safe, and efficient manner.
The package and delivery process starts with the sender preparing the package for shipment by packaging the goods securely and labeling them correctly. The package is then handed over to the delivery company, who arranges for the transportation of the package to its destination.
Various modes of transportation are used for packaging and delivery, including land, air, and sea. The mode of transportation used depends on various factors such as the distance between the sender and recipient, the size and weight of the package, and the urgency of delivery.

Whether Gr2 or Gr12 titanium circles are better depending on the specific application requirements. Both Gr2 and Gr12 titanium circles have unique properties that make them suitable for different applications.
Gr2 titanium circles are commercially pure titanium with excellent corrosion resistance, formability, and weldability. They have a high strength-to-weight ratio, making them ideal for various industrial applications, such as aerospace, medical, chemical processing, marine, and automotive industries.
On the other hand, Gr12 titanium circles are an alpha-beta alloy of titanium with an exceptional strength-to-weight ratio, high-temperature resistance, and good ductility. They are highly resistant to corrosion and are suitable for applications where high strength and elevated temperature resistance are required, such as in the aerospace industry for manufacturing engine components and structural elements, and in chemical processing and petrochemical industries.
In summary, both Gr2 and Gr12 titanium circles possess unique properties that make them suitable for different applications. Choosing between the two depends on the specific requirements of the intended application. Therefore, it is essential to consider the properties and characteristics of both grades carefully to select the appropriate one for your application.
Other related titanium plates.

Contact Us
No.11th Road of Gaoxin, Baoji, Shaanxi, P.R.China
Tel: +86-0917- 3664600
Fax: +86-0917- 3664600
Whatsapp: +8618791798690
Mail: sales@tmsalloy.com
Hot Tags: astmb265 waterjet cutting gr2 gr12 titanium circles, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China