Baoji Fairy Titanium Industry Co., Ltd. is one of the leading manufacturers and suppliers of astmb381 high strength titanium forged ring in China. Welcome to wholesale bulk high quality customized products made in China here from our factory. Good service and low price are available.
1. ASTM B381 titanium forged ring covers forging ring, disc, and flanges of titanium and titanium alloy. Titanium forging is a deformation procedure of materials through compressive stress. The process is done hot or cold. Hot forging is carried out at a temperature higher than the recrystallization temperature, usually 0.6 Tm or higher, and Tm is the melting temperature.
2. ASTM B381 Titanium Forged Flanges available information
Grade: GR1, BT1-00, GR2, BT1-0, GR5, BT6, GR7, GR12, BT1-2 BT5-1 3B.
Types: titanium forge rings, titanium discs, titanium blocks, titanium squares, titanium alloy rings, titanium alloy impellers for gas engines, titanium forgings for deep-sea engineering, etc.
Production method: ① hot forging, machining. ② hot extrusion, machining. ③Hot rolling and machining


3. ASTM B381 Titanium Forged Flanges feature high strength, high plasticity, high-pressure resistance, high-temperature resistance, wear resistance, good corrosion resistance, and good machining performance.
4. Production process: titanium ingot inspection_forging-elimination of work hardening annealing_drilling (wire cutting)-machining-stress relief annealing-internal and external surface machining-size and mechanical inspection.


| Category | Material | Dimension(mm) | Specification |
| Ti & Alloy forging ring | CP Ti, | Standard Or Customized | ASTM B381 |
| Ti-6Al-4V, Ti-6Al-4V Eli, | |||
| Ti-3Al-2.5V, | |||
| Ti-5Al-2.5Sn, Ti-5Al-2.5Sn Eli, | |||
| Ti-0.05Pd, Ti-0.2Pd, | |||
| Ti-6Al-7Nb, | |||
| Ti-13Nb-13Zr, | |||
| Ti-0.1Ru, | |||
| Ti-3Al-8V-6Cr-4Mo-4Zr, | |||
| Ti-6Al-4V-0.1Ru, | |||
| etc. |
5. Detection process: ultrasonic testing, color penetration testing, size, and mechanical properties test.
6. Application of ASTM B381 titanium forged ring: the products are widely used in pressure-resistant equipment, pressure vessel tanks, mining equipment, coal chemical equipment, and other high-pressure, wear-resistant, corrosion-resistant, non-magnetic, and high-temperature fields.
7. Tensile and yield strength according to ASTMB381
| Grade | Tensile Strength, min | Yield Strength 0.2% Offset, min or Range | Elongation in 4D, | Reduction of Area, |
| MPa | MPa | min,% | min,% | |
| F-1 | 240 | 138 | 24 | 30 |
| F-2 | 345 | 275 | 20 | 30 |
| F-2HB.C | 400 | 275 | 20 | 30 |
| F-3 | 450 | 380 | 18 | 30 |
| F-4 | 550 | 483 | 15 | 25 |
| F-5 | 895 | 828 | 10 | 25 |
| F-6 | 828 | 795 | 10 | 25 |
| F-7 | 345 | 275 | 20 | 30 |
| F-7HB.C | 400 | 275 | 20 | 30 |
| F-9 | 828 | 759 | 10 | 25 |
| F-90 | 620 | 483 | 15 | 25 |
| F-11 | 240 | 138 | 24 | 30 |
| F-12 | 483 | 345 | 18 | 25 |
| F-13 | 275 | 170 | 24 | 30 |
| F-14 | 410 | 275 | 20 | 30 |
| F-15 | 483 | 380 | 18 | 25 |
| F-16 | 345 | 275 | 20 | 30 |
| F-16HB.C | 400 | 275 | 20 | 30 |
| F-17 | 240 | 138 | 24 | 30 |
| F-18 | 620 | 483 | 15 | 25 |
| F-18D | 620 | 483 | 12 | 20 |
| F-19E | 793 | 759 | 15 | 25 |
| F-19F | 930 | 897 to 1096 | 10 | 20 |
| F-19G | 1138 | 1104 to 1276 | 5 | 20 |
| F-20E | 793 | 759 | 15 | 25 |
| F-20F | 930 | 897 to 1096 | 10 | 20 |
| F-20G | 1138 | 1104 to 1276 | 5 | 20 |
| F-21E | 793 | 759 | 15 | 35 |
| F-21F | 966 | 897 to 1096 | 10 | 30 |
| F-21G | 1172 | 1104 to 1276 | 8 | 20 |
| F-23 | 828 | 759 | 10 | 25 |
8. Why choose us
We, ASTM b381 titanium forged ring supplier in Baoji, have skillful employees with rich experiences to provide you the excellent forging parts, not only titanium ASTM b381 F2 but also F5, F7, F12 titanium, we have quick and on-time delivery to satisfy your urgent requests because we have enough titanium material stock, contact us to buy ASTM b381 titanium forge ring at sales@tmsalloy.com

Hot Tags: astmb381 high strength titanium forged ring, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China, ASTMB265 Waterjet Cutting Gr2 Gr12 Titanium Circles, Gr5 Dental Titanium Disc